journal article·2014-01-01Open access

Self-forming Al oxide barrier for nanoscale Cu interconnects created by hybrid atomic layer deposition of Cu–Al alloy

Jae-Hyung Park, Dong-Suk Han, You-Jin Kang, So-Ra Shin, Jong-Wan Park

Abstract

The authors synthesized a Cu–Al alloy by employing alternating atomic layer deposition (ALD) surface reactions using Cu and Al precursors, respectively. By alternating between these two ALD surface chemistries, the authors fabricated ALD Cu–Al alloy. Cu was deposited using bis(1-dimethylamino-2-methyl-2-butoxy) copper as a precursor and H2 plasma, while Al was deposited using trimethylaluminum as the precursor and H2 plasma. The Al atomic percent in the Cu–Al alloy films varied from 0 to 15.6 at. %. Transmission electron microscopy revealed that a uniform Al-based interlayer self-formed at the interface after annealing. To evaluate the barrier properties of the Al-based interlayer and adhesion between the Cu–Al alloy film and SiO2 dielectric, thermal stability and peel-off adhesion tests were performed, respectively. The Al-based interlayer showed similar thermal stability and adhesion to the reference Mn-based interlayer. Our results indicate that Cu–Al alloys formed by alternating ALD are suitable seed layer materials for Cu interconnects.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Copper Interconnects and Reliability · Semiconductor materials and devices · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Division of Nanoscale Semiconductor Engineering, Hanyang University , Seoul 133-791, South Korea

Division of Materials Science and Engineering, Hanyang University , Seoul 133-791, South Korea

References (28)

Show source-provided references
1. 2011
2. , J. Electrochem. Soc. · 2006 · 153 · C78710.1149/1.2338632 ↗
3. J. Vac. Sci. Technol. B. · 2007 · 25 · 258110.1116/1.2779050 ↗
4. Phys. Rev. B. · 2002 · 66 · 07541410.1103/PhysRevB.66.075414 ↗
5. J. Vac. Sci. Technol. B. · 2004 · 22 · 24010.1116/1.1642639 ↗
6. APL Mater. · 2013 · 1 · 04210510.1063/1.4822441 ↗
7. Jpn. J. Appl. Phys. · 2012 · 51 · 04DB0610.1143/JJAP.51.04DB06 ↗
8. J. Vac. Sci. Technol. A. · 2013 · 31 · 01A13710.1116/1.4769204 ↗
9. Microelectron. Eng. · 2013 · 110 · 2910.1016/j.mee.2013.03.176 ↗
10. Appl. Phys. Lett. · 2013 · 102 · 11191010.1063/1.4798337 ↗
11. Thin Solid Films · 1995 · 262 · 23410.1016/0040-6090(95)05837-0 ↗
12. J. Appl. Phys. · 1994 · 75 · 362710.1063/1.356075 ↗
13. Appl. Phys. Lett. · 1994 · 64 · 289710.1063/1.111408 ↗
14. Thin Solid Films · 1998 · 335 · 4910.1016/S0040-6090(98)00878-5 ↗
15. 2004
16. Microelectron. Eng. · 2008 · 85 · 213710.1016/j.mee.2008.04.004 ↗
17. IEEE Trans. Electron Devices · 2007 · 54 · 186710.1109/TED.2007.901265 ↗
18. 1953
19. 1998
20. Thin Solid Films · 2010 · 518 · 164810.1016/j.tsf.2009.11.075 ↗
21. 1998 · 107
22. Thin Solid Films. · 2012 · 521 · 14610.1016/j.tsf.2012.02.015 ↗
23. AIP Conf. Proc. · 2006 · 817 · 4310.1063/1.2173530 ↗
24. J. Appl. Phys. · 2003 · 94 · 160510.1063/1.1589593 ↗
26. J. Vac. Sci. Technol. A. · 2001 · 19 · 264210.1116/1.1399323 ↗
27. Microelectron. Eng. · 2000 · 50 · 54710.1016/S0167-9317(99)00326-3 ↗
28. J. Electrochem. Soc. · 2004 · 151 · C75310.1149/1.1809576 ↗