journal article·2011-01-01

DC reactive magnetron sputtering, annealing, and characterization of CuAlO2 thin films

Blake L. Stevens, Cathleen A. Hoel, Carolyn Swanborg, Yang Tang, Chuanle Zhou, Matthew Grayson, Kenneth R. Poeppelmeier, Scott A. Barnett

Publisher page

Abstract

CuAlO x thin films were prepared at three substrate temperatures (TS=60, 300, and 600 °C) and two oxygen partial pressures (PO2=0.5 and 2 mTorr) via dc reactive magnetron sputtering from Cu–Al 50–50 at. % alloy targets and subsequent annealing. As-deposited films with PO2=0.5 mTorr were oxygen deficient; although the delafossite structure formed upon annealing, electrical properties were poor. Films deposited with PO2=2 mTorr transformed into the delafossite structure and exhibited p-type conductivity after annealing under N2 at temperatures TA≥750 °C. Conductivity generally increased with increasing TS and decreasing TA. A special case of PO2=2 mTorr and low TS (60 °C) resulted in a partially crystalline oxide phase that transformed into the delafossite structure at TA=700 °C and yielded the highest conductivity of 1.8 S cm−1. In general, a TA near the phase formation boundary led to an increase in conductivity. Low-temperature hydrothermal annealing was also investigated and shown to produce mixed phase films exhibiting the delafossite structure along with CuO, AlOOH, and Al2O3.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Copper-based nanomaterials and applications · ZnO doping and properties · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Northwestern University Department of Materials Science and Engineering, , Evanston, Illinois 60208

Northwestern University Department of Chemistry, , Evanston, Illinois 60208

Northwestern University Electrical Engineering and Computer Science, , Evanston, Illinois 60208

References (28)

Show source-provided references
1. MRS Bull. · 2000 · 25 · 15
2. MRS Bull. · 2000 · 25 · 28
3. Nature (London) · 1997 · 389 · 93910.1038/40087 ↗
4. Chem. Mater. · 2006 · 18 · 710.1021/cm051791c ↗
5. Electrochem. Solid-State Lett. · 1999 · 2 · 65410.1149/1.1390938 ↗
6. Thin Solid Films · 2003 · 445 · 29910.1016/S0040-6090(03)01175-1 ↗
7. J. Mater. Sci. · 2009 · 44 · 159410.1007/s10853-008-3229-2 ↗
8. Mater. Lett. · 2004 · 58 · 1010.1016/S0167-577X(03)00395-1 ↗
9. J. Mater. Sci.: Mater. Electron. · 2006 · 17 · 61510.1007/s10854-006-0007-2 ↗
10. J. Phys. Chem. Solids · 2003 · 64 · 167110.1016/S0022-3697(03)00194-X ↗
11. Prog. Cryst. Growth Charact. Mater. · 2005 · 50 · 5210.1016/j.pcrysgrow.2005.10.001 ↗
12. Thin Solid Films · 2003 · 440 · 510.1016/S0040-6090(03)00817-4 ↗
13. Jpn. J. Appl. Phys., Part 1 · 2007 · 46 · 35110.1143/JJAP.46.351 ↗
14. J. Electrochem. Soc. · 2007 · 154 · H83810.1149/1.2756991 ↗
15. J. Vac. Sci. Technol. A · 1992 · 10 · 7510.1116/1.578069 ↗
16. Science · 2002 · 297 · 6510.1126/science.1072009 ↗
17. 2002 · 216
18. Thin Solid Films · 2002 · 411 · 12910.1016/S0040-6090(02)00201-8 ↗
19. J. Am. Ceram. Soc. · 1994 · 77 · 203610.1111/j.1151-2916.1994.tb07094.x ↗
20. J. Am. Ceram. Soc. · 1975 · 58 · 19210.1111/j.1151-2916.1975.tb11441.x ↗
21. Physica B · 2005 · 370 · 26410.1016/j.physb.2005.09.022 ↗
22. J. Am. Ceram. Soc. · 1972 · 55 · 39510.1111/j.1151-2916.1972.tb11320.x ↗
23. J. Solid State Chem. · 1981 · 40 · 17010.1016/0022-4596(81)90377-7 ↗
24. Z. Anorg. Allg. Chem. · 1986 · 543 · 7310.1002/zaac.19865431209 ↗
25. 1971 · 34
26. Thin Solid Films · 2008 · 516 · 813010.1016/j.tsf.2008.04.020 ↗
27. 1984 · 4159
28. J. Appl. Phys. · 2000 · 88 · 415910.1063/1.1308103 ↗