Investigating the effects of proton exchange membrane fuel cell conditions on carbon supported platinum electrocatalyst composition and performance
Source abstract
Abstract
Changes that carbon-supported platinum electrocatalysts undergo in a proton exchange membrane fuel cell environment were simulated by ex situ heat treatment of catalyst powder samples at 150 °C and 100% relative humidity. In order to study modifications that are introduced to chemistry, morphology, and performance of electrocatalysts, XPS, HREELS and three-electrode rotating disk electrode experiments were performed. Before heat treatment, graphitic content varied by 20% among samples with different types of carbon supports, with distinct differences between bulk and surface compositions within each sample. Following the aging protocol, the bulk and surface chemistry of the samples were similar, with graphite content increasing or remaining constant and Pt-carbide decreasing for all samples. From the correlation of changes in chemical composition and losses in performance of the electrocatalysts, we conclude that relative distribution of Pt particles on graphitic and amorphous carbon is as important for electrocatalytic activity as the absolute amount of graphitic carbon present.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electrocatalysts for Energy Conversion · Fuel Cells and Related Materials · Advanced battery technologies research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
University of New Mexico Chemical and Nuclear Engineering Department, UNM Center for Emerging Energy Technologies, , Albuquerque, New Mexico 87131
Ballard Power Systems, Burnaby British Columbia , V5J 5J8 Canada
References (24)
Show source-provided references
1. Chem. Rev. · 2007 · 107 · 390410.1021/cr050182l ↗
2. J. Alloy Compd. · 2008 · 461 · 25310.1016/j.jallcom.2007.06.077 ↗
3. J. Power Sources · 2007 · 172 · 13310.1016/j.jpowsour.2007.07.049 ↗
4. J. Power Sources · 2007 · 172 · 14510.1016/j.jpowsour.2007.07.048 ↗
5. Int. J. Hydrogen Energy · 1999 · 24 · 110710.1016/S0360-3199(98)00172-4 ↗
6. ECS Trans. · 2007 · 11 · 98110.1149/1.2781011 ↗
7. Int. J. Hydrogen Energy · 2010 · 35 · 758010.1016/j.ijhydene.2010.04.147 ↗
8. Int. J. Hydrogen Energy · 2009 · 34 · 897410.1016/j.ijhydene.2009.08.094 ↗
9. J. Electrochem. Soc. · 2007 · 154 · B100610.1149/1.2764240 ↗
10. J. Power Sources · 1999 · 84 · 16710.1016/S0378-7753(99)00333-X ↗
11. J. Phys. Chem. C · 2011 · 115 · 216210.1021/jp109975s ↗
12. J. Power Sources · 2011 · 196 · 524010.1016/j.jpowsour.2010.11.016 ↗
13. J. Fuel Cell Sci. Technol. · 2006 · 3 · 42810.1115/1.2349524 ↗
14. ECS Trans. · 2010 · 33 · 128110.1149/1.3484621 ↗
15. J. Electrochem. Soc. · 2009 · 156 · B91310.1149/1.3139963 ↗
16. ECS Trans. · 2006 · 3 · 78310.1149/1.2356198 ↗
17. ECS Trans. · 2006 · 3 · 81110.1149/1.2356200 ↗
18. ECS Trans. · 2006 · 3 · 79710.1149/1.2356199 ↗
19. J. Electrochem. Soc. · 2005 · 152 · A225610.1149/1.2050347 ↗
20. ECS Trans. · 2006 · 3 · 74310.1149/1.2356194 ↗
21. J. Power Sources · 2009 · 194 · 84710.1016/j.jpowsour.2009.06.059 ↗
22. J. Electrochem. Soc. · 2005 · 152 · A230910.1149/1.2097361 ↗
23. J. Phys. Chem. A · 2009 · 113 · 1387110.1021/jp905639d ↗
24. Thin Solid Films · 2005 · 488 · 28310.1016/j.tsf.2005.04.025 ↗