journal article·2020-03-01Open access

AlOx surface passivation of black silicon by spatial ALD: Stability under light soaking and damp heat exposure

Ismo T. S. Heikkinen, George Koutsourakis, Sauli Virtanen, Marko Yli-Koski, Sebastian Wood, Ville Vähänissi, Emma Salmi, Fernando A. Castro, Hele Savin

Abstract

Scientific breakthroughs in silicon surface passivation have enabled commercial high-efficiency photovoltaic devices making use of the black silicon nanostructure. In this study, the authors report on factors that influence the passivation stability of black silicon realized with industrially viable spatial atomic layer deposited (SALD) aluminum oxide (AlOx) under damp heat exposure and light soaking. Damp heat exposure conditions are 85 °C and 85% relative humidity, and light soaking is performed with 0.6 sun illumination at 75 °C. It is demonstrated that reasonably thick (20 nm) passivation films are required for both black and planar surfaces in order to provide stable surface passivation over a period of 1000 h under both testing conditions. Both surface textures degrade at similar rates with 5 and 2 nm thick films. The degradation mechanism under damp heat exposure is found to be different from that in light soaking. During damp heat exposure, the fixed charge density of AlOx is reduced, which decreases the amount of field-effect passivation. Degradation under light soaking, on the other hand, is likely to be related to interface defects between silicon and the passivating film. Finally, a thin chemically grown SiOx layer at the interface between the AlOx film and the silicon surface is shown to significantly increase the passivation stability under both light soaking and damp heat exposure. The results of this study provide valuable insights into surface passivation degradation mechanisms on nanostructured silicon surfaces and pave the way for the industrial production of highly stable black silicon devices.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and devices · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Electronics and Nanoengineering, Aalto University 1 , Tietotie 3, FI-02150 Espoo, Finland

National Physical Laboratory 2 , Hampton Road, Teddington TW11 0LW, United Kingdom

Beneq Oy 3 , Olarinluoma 9, FI-02200 Espoo, Finland

Funding

Academy of Finland · European Metrology Programme for Innovation and Research · Department for Business, Energy and Industrial Strategy · Walter Ahlströmin Säätiö · Sähkötekniikan Korkeakoulu, Aalto-yliopisto

References (34)

Show source-provided references
1. Nat. Photonics · 2016 · 10 · 77710.1038/nphoton.2016.226 ↗
2. Nat. Nanotechnol. · 2015 · 10 · 62410.1038/nnano.2015.89 ↗
3. J. Appl. Phys. · 2008 · 104 · 11370310.1063/1.3021091 ↗
4. Phys. Status Solidi A · 2017 · 214 · 170023910.1002/pssa.201700293 ↗
5. IEEE J. Photovoltaics · 2013 · 3 · 9010.1109/JPHOTOV.2012.2210031 ↗
6. Sol. Energy Mater. Sol. Cells · 2015 · 142 · 2910.1016/j.solmat.2015.05.027 ↗
7. Elfys Inc
8. PVTech
9. PVTech
10. 2018
11. AIP Conf. Proc. · 2018 · 1999 · 05000710.1063/1.5049297 ↗
12. J. Vac. Sci. Technol. A · 2012 · 30 · 04080210.1116/1.4728205 ↗
13. J. Vac. Sci. Technol. A · 2012 · 30 · 01080210.1116/1.3670745 ↗
14. Sol. Energy Mater. Sol. Cells · 2015 · 143 · 8310.1016/j.solmat.2015.06.015 ↗
15. Energy Procedia · 2016 · 92 · 21110.1016/j.egypro.2016.07.061 ↗
16. Sol. Energy Mater. Sol. Cells · 2018 · 188 · 11210.1016/j.solmat.2018.08.019 ↗
17. D. Sperber, “Bulk and surface related degradation phenomena in monocrystalline silicon at elevated temperature and illumination,” doctoral dissertation (University of Konstanz, 2019).
18. IEEE J. Photovoltaics · 2017 · 7 · 119710.1109/JPHOTOV.2017.2713411 ↗
19. IEEE J. Photovoltaics · 2019 · 9 · 9710.1109/JPHOTOV.2018.2878791 ↗
20. 2013
21. Phys. Status Solidi A · 2015 · 212 · 27410.1002/pssa.201431256 ↗
22. Int. J. Heat Mass Transfer · 2016 · 96 · 18910.1016/j.ijheatmasstransfer.2016.01.034 ↗
23. Int. J. Heat Mass Transfer · 2019 · 144 · 11864210.1016/j.ijheatmasstransfer.2019.118642 ↗
24. Phys. Status Solidi RRL · 2016 · 10 · 44310.1002/pssr.201600080 ↗
25. J. Appl. Phys. · 2002 · 92 · 716810.1063/1.1522811 ↗
26. Energy Procedia · 2017 · 124 · 28210.1016/j.egypro.2017.09.300 ↗
27. Appl. Phys. Lett. · 1996 · 69 · 251010.1063/1.117723 ↗
28. Energy Procedia · 2012 · 15 · 13510.1016/j.egypro.2012.02.016 ↗
29. AIP Conf. Proc · 2001 · 550 · 22010.1063/1.1354401 ↗
30. Curr. Appl. Phys · 2004 · 4 · 10810.1016/j.cap.2003.10.008 ↗
31. J. Appl. Phys. · 2013 · 113 · 02450910.1063/1.4775595 ↗
32. AIP Conf. Proc. · 2019 · 2147 · 05000310.1063/1.5123852 ↗
33. J. Vac. Sci. Technol. A · 2015 · 33 · 01A123-110.1116/1.4901456 ↗
34. IEEE Trans. Electron Devices · 1997 · 44 · 16010.1109/16.554806 ↗