Chemical vapor deposition of sp2-boron nitride on Si(111) substrates from triethylboron and ammonia: Effect of surface treatments
Source abstract
Abstract
Thin films of the sp2-hybridized polytypes of boron nitride (BN) are interesting materials for several electronic applications such as UV devices. Deposition of epitaxial sp2-BN films has been demonstrated on several technologically important semiconductor substrates such as SiC and Al2O3 and where controlled thin film growth on Si would be beneficial for integration of sp2-BN in many electronic device systems. The authors investigate the growth of BN films on Si(111) by chemical vapor deposition from triethylboron [B(C2H5)3] and ammonia (NH3) at 1300 °C with focus on treatments of the Si(111) surface by nitridation, carbidization, or nitridation followed by carbidization prior to BN growth. Fourier transform infrared spectroscopy shows that the BN films deposited exhibit sp2 bonding. X-ray diffraction reveals that the sp2-BN films predominantly grow amorphous on untreated and pretreated Si(111), but with diffraction data showing that turbostratic BN can be deposited on Si(111) when the formation of Si3N4 is avoided. The authors accomplish this condition by combining the nitridation procedure with reactions from the walls on which BxC had previously been deposited.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Graphene research and applications · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Physics, Chemistry and Biology (IFM), Linköping University , SE-581 83 Linköping, Sweden
Funding
Swedish government strategic area in materials science · Stiftelsen för Strategisk Forskning
References (51)
Show source-provided references
1. Acta Crystallogr. · 1952 · 5 · 35610.1107/S0365110X52001064 ↗
2. Proc. Japan Acad. · 1985 · 61 · 45910.2183/pjab.61.459 ↗
3. Nat. Mater. · 2004 · 3 · 40410.1038/nmat1134 ↗
4. Science · 2007 · 317 · 93210.1126/science.1144216 ↗
5. Appl. Phys. Lett. · 2016 · 109 · 11350110.1063/1.4962831 ↗
6. Proc. SPIE · 2016 · 9968 · 99680S10.1117/12.2239079 ↗
7. Appl. Phys. Lett. · 2016 · 109 · 07210110.1063/1.4960522 ↗
8. Appl. Phys. Lett. · 2011 · 98 · 26210310.1063/1.3604012 ↗
9. Appl. Phys. Lett. · 2011 · 98 · 24210510.1063/1.3599708 ↗
10. J. Mater. Res. · 2014 · 29 · 45910.1557/jmr.2013.323 ↗
11. Phys. Status Solidi Rapid Res. Lett. · 2011 · 5 · 39710.1002/pssr.201105410 ↗
12. Cryst. Growth Des. · 2012 · 12 · 321510.1021/cg300364y ↗
13. CrystEngComm · 2014 · 16 · 543010.1039/C4CE00381K ↗
14. Jpn. J. Appl. Phys. · 2016 · 55 · 05FD0910.7567/JJAP.55.05FD09 ↗
15. J. Vac. Sci. Technol. A. · 2019 · 37 · 02060310.1116/1.5085192 ↗
16. Jpn. J. Appl. Phys. · 2007 · 46 · 255410.1143/JJAP.46.2554 ↗
17. Mater. Res. Express · 2017 · 4 · 01500710.1088/2053-1591/aa54d5 ↗
18. J. Electrochem. Soc. · 1968 · 115 · 42310.1149/1.2411238 ↗
19. J. Electrochem. Soc. · 1975 · 122 · 167110.1149/1.2134107 ↗
20. J. Electrochem. Soc. · 1979 · 126 · 195110.1149/1.2128833 ↗
21. J. Electrochem. Soc. · 1980 · 127 · 39910.1149/1.2129678 ↗
22. J. Electrochem. Soc. · 1980 · 127 · 154610.1149/1.2129947 ↗
23. Vacuum · 1994 · 45 · 102910.1016/0042-207X(94)90014-0 ↗
24. J. Electrochem. Soc. · 1985 · 132 · 175710.1149/1.2114206 ↗
25. Thin Solid Films · 2012 · 520 · 588910.1016/j.tsf.2012.05.004 ↗
26. J. Phys. IV · 1995 · C5-76110.1051/jphyscol:1995590 ↗
27. Surf. Coat. Technol. · 2011 · 205 · 373610.1016/j.surfcoat.2011.01.032 ↗
28. Chem. Vap. Deposition · 2012 · 18 · 24910.1002/cvde.201106969 ↗
29. Thin Solid Films · 2018 · 664 · 10610.1016/j.tsf.2018.08.020 ↗
30. CrystEngComm · 2013 · 15 · 45510.1039/C2CE26423D ↗
31. Phys. Rev. · 1966 · 146 · 54310.1103/PhysRev.146.543 ↗
32. Phys. Rev. · 1967 · 155 · 103910.1103/PhysRev.155.1039 ↗
33. Phys. Rev. B · 1984 · 30 · 605110.1103/PhysRevB.30.6051 ↗
34. Diamond Relat. Mater. · 1994 · 3 · 83110.1016/0925-9635(94)90279-8 ↗
35. Phys. Rev. B · 1982 · 25 · 115110.1103/PhysRevB.25.1151 ↗
36. J. Non Cryst. Solids · 1981 · 43 · 710.1016/0022-3093(81)90169-1 ↗
37. J. Electrochem. Soc. · 1983 · 130 · 156010.1149/1.2120034 ↗
38. J. Vac. Sci. Technol. A · 2018 · 36 · 03080110.1116/1.5024314 ↗
39. Acta Crystallogr. · 1965 · 18 · 99210.1107/S0365110X65002414 ↗
40. Carbon · 1995 · 33 · 139910.1016/0008-6223(95)00086-S ↗
41. Carbon · 2003 · 41 · 158510.1016/S0008-6223(03)00116-7 ↗
42. Carbon · 2007 · 45 · 168610.1016/j.carbon.2007.03.038 ↗
43. Physica B · 2014 · 439 · 2910.1016/j.physb.2013.10.068 ↗
44. 1961
45. J. Am. Ceram. Soc. · 2002 · 85 · 213110.1111/j.1151-2916.2002.tb00420.x ↗
46. 1979 · 9:4
47. J. Phys. Chem. Ref. Data · 1998 · 27 · 80710.1063/1.556022 ↗
48. 2003
49. J. Theor. Comput. Chem. · 2008 · 7 · 126910.1142/S0219633608004532 ↗
50. J. Cryst. Growth · 2003 · 253 · 2610.1016/S0022-0248(03)00971-0 ↗
51. See supplementary material at https://doi.org/10.1116/1.5145287 for FTIR reflectance spectra and pole figures of BN films, phi-scans and top-view SEM for SiC, GID and top-view SEM for Si3N4, XRD and FTIR for r-BxC.