Atomic layer chemical vapor deposition of zirconium silicate films with a precursor combination of ZrCl4 and tetra-n-butyl orthosilicate (TBOS) was studied for high dielectric gate insulators. The effect of deposition conditions, such as deposition temperature, pulse time for purge and precursor injection on the deposition rate per cycle, and composition of the film were studied. At 400 °C, the growth rate saturated to 1.35 Å/cycle above 500 sccm of the argon purge flow rate. The growth rate, composition ratio ((Zr/Zr+Si)), and impurity contents (carbon and chlorine) saturated with the increase of the injection time of ZrCl4 and TBOS and decreased with the increased deposition temperature from 300 to 500 °C. The growth rate, composition ratio, carbon, and chlorine contents of the Zr silicate thin films deposited at 500 °C were 1.05 Å/cycle, 0.23, 1.1 at. %, and 2.1 at. %, respectively. It appeared that by using only zirconium chloride and silicon alkoxide sources, the content of carbon and chlorine impurities could not be lowered below 1%. It was also found that the incorporation rate of metal from halide source was lower than alkoxide source.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Catalytic Processes in Materials Science · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemical Engineering, Laboratory for Advanced Molecular Processing, Pohang University of Science and Technology, Pohang 790-784, Korea

Preceding Process Development Team, Samsung Electronics Co., Ltd. San #24, Nongseo-Ree, Kiheung-Eup, Yongin-City, Kyonggi-Do 499-900, Korea

References (15)

Show source-provided references
1. Appl. Phys. Lett. · 1998 · 72 · 283510.1063/1.121473 ↗
2. J. Am. Chem. Soc. · 1999 · 121 · 522010.1021/ja984446f ↗
3. Phys. Rev. Lett. · 1998 · 81 · 301410.1103/PhysRevLett.81.3014 ↗
4. Appl. Phys. Lett. · 2000 · 76 · 17610.1063/1.125694 ↗
5. J. Electrochem. Soc. · 2002 · 149 · G8910.1149/1.1425798 ↗
6. Appl. Phys. Lett. · 2000 · 77 · 188510.1063/1.1310635 ↗
7. J. Appl. Phys. · 2001 · 89 · 524310.1063/1.1361065 ↗
8. Appl. Phys. Lett. · 2000 · 76 · 11210.1063/1.125673 ↗
9. Science · 2000 · 288 · 31910.1126/science.288.5464.319 ↗
10. Chem. Mater. · 2001 · 13 · 246310.1021/cm010145k ↗
11. J. Electrochem. Soc. · 1995 · 142 · 67610.1149/1.2044122 ↗
12. Thin Solid Films · 1993 · 225 · 28010.1016/0040-6090(93)90170-T ↗
13. Surf. Sci. · 1995 · 334 · 13510.1016/0039-6028(95)00471-8 ↗
14. Thin Solid Films · 1999 · 340 · 11010.1016/S0040-6090(98)01356-X ↗
15. J. Appl. Phys. · 2001 · 90 · 180110.1063/1.1382851 ↗