Reactive-sputter deposition and structure of RuO2 films on sapphire and strontium titanate
Source abstract
Abstract
Metallic films of RuO2 were deposited by reactive-sputtering deposition on single crystal substrates of Al2O3 (0001) and SrTiO3 (100) at room temperature and 450 °C. Measurement of the characteristic hysteresis loop revealed that the target’s transition from a metal to a metal oxide surface occurred at a very high O2/Ar ratio (88%) under our experimental conditions. The hysteretical behavior of the transition was evaluated experimentally and was modeled. Resonance-enhanced Rutherford backscattering spectrometry established that the films deposited at 450 °C had an oxygen to ruthenium ratio of 1.97, while a slightly higher value of 2.08 was observed for the films grown at room temperature. The latter films were amorphous, whereas those grown at 450 °C exhibited a highly oriented polycrystalline microstructure. On SrTiO3 (100), the RuO2 (100) plane is parallel to the substrate surface, but no in-plane orientation was found. The same face, RuO2 (100), was also parallel to the surface of Al2O3 (0001), and the [001] direction of individual grains of RuO2 aligned with the three 〈1̄010〉 directions of the substrate to produce a threefold mosaic microstructure.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic and Structural Properties of Oxides · Semiconductor materials and devices · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemistry and Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, Minnesota 55455
References