journal article·1992-07-01

Particle contamination during sputter deposition of W–Ti films

C. E. Wickersham, J. E. Poole, J. J. Mueller

Publisher page

Abstract

Particle contamination during sputter deposition of W–Ti films depends upon the target density, the amount of Ti rich β(Ti,W) in the target, the target impurity content, and the film compressive stress. Particle contamination densities decrease from ∼1.5 cm−2 to less than 0.1 cm−2 as the sputtering target microstructure is changed from a 76% dense multiphase mixture of Ti rich β(Ti,W) and β-W to a 99% dense two phase combination of β-W and α-Ti. A process map is provided to guide the selection of optimum powder compaction process for W–Ti targets. We propose that particle emission from the Ti rich β(W–Ti) phase in W–Ti sputtering targets occurs by argon bombardment induced compressive stress fracture of the Ti rich β(Ti,W) phase. Particle contamination density increases at a rate of 1.5×10−4 particles/cm2 for each (parts per million by weight) of target impurity. An inverse relationship between the total deposited film thickness and the film compressive strain was found. Increasing the W–Ti film compressive strain reduces the film thickness at which stress fracture (flaking) of the film deposited on the system shields occurs. A reduced stress fracture thickness means that particle emission from the system shielding will occur at an early stage as film accumulates on the exposed shielding.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

TOSOH SMD, Inc., 3515 Grove City Road, Grove City, Ohio 43123

References

Reference metadata was not supplied for this record.