Improving the thermal stability of nickel monosilicide thin films by combining annealing with the use of an interlayer and a capping layer
Source abstract
Abstract
The authors investigated the effects of preannealing a 2-nm-thick Pd interlayer and a 20-nm-thick TiN capping layer on the electrical and thermal stability of nickel silicides as a function of the annealing temperature. The preannealed samples (prepoly-Si) produce lower sheet resistances compared to the samples without preannealing. For the preannealed samples, NiSi remains stable up to 600 °C. Transmission electron microscopy results show that the preannealed samples have a higher resistance against layer inversion. The addition of a Pd interlayer at the Ni film/prepoly-Si interface increases the formation temperature of NiSi2 to 900 °C. The use of the capping layer on the Pd-interlayered prepoly-Si samples improves the electrical and morphological stabilities of NiSi. The possible mechanisms for the preannealing and interlayer-induced improvement of the thermal stabilities of the Ni-silicide samples are discussed in terms of grain growth and simple thermodynamic relations.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Semiconductor materials and devices · Silicon Carbide Semiconductor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Korea University Department of Nano Semiconductor Engineering, , Seoul 136-713, Korea
Korea University Department of Materials Science and Engineering, , Seoul 136-713, Korea
Chonbuk National University Semiconductor Physics Research Center, School of Semiconductor and Chemical Engineering, , Jeonju 561-756, Korea
References (23)
Show source-provided references
1. J. Phys.: Condens. Matter · 2003 · 15 · 193510.1088/0953-8984/15/12/310 ↗
2. Microelectron. Eng. · 2003 · 70 · 14410.1016/S0167-9317(03)00380-0 ↗
3. Crit. Rev. Solid State Mater. Sci. · 2003 · 28 · 110.1080/10408430390802431 ↗
4. Microelectron. Eng. · 2003 · 70 · 15810.1016/S0167-9317(03)00370-8 ↗
5. Thin Solid Films · 1999 · 347 · 20110.1016/S0040-6090(99)00004-8 ↗
6. Mater. Chem. Phys. · 1996 · 46 · 20910.1016/S0254-0584(97)80015-6 ↗
7. Mater. Sci. Eng. R. · 1996 · 16 · 4310.1016/0927-796X(95)00186-7 ↗
8. Thin Solid Films · 1994 · 253 · 47910.1016/0040-6090(94)90370-0 ↗
9. Curr. Appl. Phys. · 2010 · 10 · 4110.1016/j.cap.2009.04.011 ↗
10. J. Appl. Phys. · 2005 · 98 · 03352610.1063/1.2005380 ↗
11. Thin Solid Films · 2004 · 462–463 · 14610.1016/j.tsf.2004.05.091 ↗
12. J. Electrochem. Soc. · 2002 · 149 · G50510.1149/1.1494828 ↗
13. Microelectron. Eng. · 2007 · 84 · 180110.1016/j.mee.2007.01.198 ↗
14. J. Electrochem. Soc. · 2006 · 153 · G3510.1149/1.2130695 ↗
15. Jpn. J. Appl. Phys., Part 2 · 1990 · 29 · L232910.1143/JJAP.29.L2329 ↗
16. Phys. Status Solidi A · 1984 · 81 · 12310.1002/pssa.2210810111 ↗
17. 1993 · 192
18. IEEE Electron Device Lett. · 1999 · 20 · 57210.1109/55.798047 ↗
19. Jpn. J. Appl. Phys., Part 1 · 2002 · 41 · 196910.1143/JJAP.41.1969 ↗
20. IEEE Trans. Electron Devices · 1995 · 42 · 91510.1109/16.381988 ↗
21. J. Appl. Phys. · 1984 · 55 · 420810.1063/1.333021 ↗
22. J. Phase Equilib. · 1991 · 12 · 34910.1007/BF02649925 ↗
23. J. Mater. Res. · 1988 · 3 · 16710.1557/JMR.1988.0167 ↗