Enhancing mechanical properties and tribocorrosion resistance of TC4 alloys via plasma nitriding
Source abstract
Abstract
TC4 alloys were nitrided in N2: Ar plasma by a nitriding furnace to improve the hardness and tribocorrosion resistance of the titanium alloy. The effect of nitriding temperature on the microstructure and properties of the TC4 alloy was elucidated. The results show that with an increase in the nitriding temperature, the hardness and elastic modulus of the nitrided TC4 alloy as well as the thickness of the nitriding layer increase. Compared with untreated TC4, the nitrided TC4 alloys exhibit better mechanical properties, corrosion resistance, and tribocorrosion resistance due to the formation of α-Ti(N), Ti2N, and TiN. Therein, the tribocorrosion rate of the TC4 alloy at a nitriding temperature of 800 °C decreases to 1.66 × 10−5 mm3/(N m), decreased by 89.4% over untreated TC4 alloy. The enhancement in tribocorrosion properties of the nitrided TC4 alloy is attributed to the presence of nitride with high hardness and tribochemical reaction at the interface between Si3N4 and the matrix.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Shandong Laboratory of Advanced Materials and Green Manufacturing at Yantai 1 , Yantai 264006,
State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences 2 , Lanzhou 730000,
College of Nuclear Equipment and Nuclear Engineering, Yantai University 3 , Yantai 264005,
Funding
the National Natural Science Foundation of China · The Taishan Scholars Program
References (31)
Show source-provided references
1. Mater. Sci. Eng. A · 1999 · 263 · 11210.1016/S0921-5093(98)01180-0 ↗
2. Mater. Des. · 2023 · 233 · 11228810.1016/j.matdes.2023.112288 ↗
3. Corros. Sci. · 2024 · 239 · 11240010.1016/j.corsci.2024.112400 ↗
4. J. Alloy. Compd. · 2024 · 971 · 17267810.1016/j.jallcom.2023.172678 ↗
5. Corros. Sci. · 2020 · 165 · 10838510.1016/j.corsci.2019.108385 ↗
6. Vacuum · 2023 · 216 · 11246310.1016/j.vacuum.2023.112463 ↗
7. Appl. Surf. Sci. · 2018 · 457 · 91410.1016/j.apsusc.2018.06.248 ↗
8. Wear · 2024 · 550–551 · 20542310.1016/j.wear.2024.205423 ↗
9. Mater. Today Commun. · 2024 · 39 · 10869710.1016/j.mtcomm.2024.108697 ↗
10. Chem. Phys. Lett. · 2024 · 841 · 14117010.1016/j.cplett.2024.141170 ↗
11. Heliyon · 2024 · 10 · e2377910.1016/j.heliyon.2023.e23779 ↗
12. Vacuum · 2023 · 208 · 11173710.1016/j.vacuum.2022.111737 ↗
13. Surf. Coat. Technol. · 2023 · 464 · 12954410.1016/j.surfcoat.2023.129544 ↗
14. Appl. Surf. Sci. · 2023 · 617 · 15661410.1016/j.apsusc.2023.156614 ↗
15. Surf. Coat. Technol. · 2024 · 483 · 13080610.1016/j.surfcoat.2024.130806 ↗
16. J. Alloy. Compd. · 2024 · 989 · 17441810.1016/j.jallcom.2024.174418 ↗
17. Ceram. Int. · 2022 · 48 · 2147310.1016/j.ceramint.2022.04.115 ↗
18. Surf. Coat. Technol. · 2023 · 475 · 13014910.1016/j.surfcoat.2023.130149 ↗
19. Surf. Eng. · 1986 · 2 · 13310.1179/sur.1986.2.2.133 ↗
20. Surf. Coat. Technol. · 2006 · 201 · 232010.1016/j.surfcoat.2006.03.045 ↗
21. Vacuum · 2024 · 221 · 11294510.1016/j.vacuum.2023.112945 ↗
22. Surf. Coat. Technol. · 2024 · 477 · 13038110.1016/j.surfcoat.2024.130381 ↗
23. Surf. Coat. Technol. · 2023 · 456 · 12923110.1016/j.surfcoat.2023.129231 ↗
24. Surf. Coat. Technol. · 2022 · 436 · 12832710.1016/j.surfcoat.2022.128327 ↗
25. Mater. Today Commun. · 2022 · 31 · 10374610.1016/j.mtcomm.2022.103746 ↗
26. Surf. Coat. Technol. · 2015 · 264 · 3210.1016/j.surfcoat.2015.01.029 ↗
27. Wear · 2023 · 526–527 · 20493110.1016/j.wear.2023.204931 ↗
28. Surf. Coat. Technol. · 2018 · 354 · 8310.1016/j.surfcoat.2018.09.014 ↗
29. Corros. Sci. · 2004 · 46 · 91710.1016/S0010-938X(03)00188-4 ↗
30. J. Phys. Chem. C · 2020 · 124 · 2007910.1021/acs.jpcc.0c04613 ↗
31. Wear · 2012 · 288 · 2710.1016/j.wear.2012.03.001 ↗