High rate deposition of photocatalytic TiO2 films with high activity by hollow cathode gas-flow sputtering method
Source abstract
Abstract
Photocatalytic TiO2 films were deposited by a hollow cathode gas-flow sputtering method using two Ti metal targets mounted parallel to each other. The Ar and O2 flow rates were 3000 and 0–50SCCM (SCCM denotes cubic centimeter per minute at STP), respectively, and total gas pressure during the deposition was maintained at 45Pa. The highest deposition rate for the photocatalytic TiO2 films was 162nm∕min at 30SCCM of O2 flow. The as-deposited films and postannealed films, annealed in air at 300°C for 1h, were used to carry out photocatalytic decomposition of acetaldehyde (CH3CHO). In particular, the postannealed films showed extremely high photocatalytic activity compared to the photocatalytic activity of films deposited by conventional reactive sputtering.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced Photocatalysis Techniques · TiO2 Photocatalysis and Solar Cells · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Aoyama Gakuin University Graduate School of Science and Engineering, , 5-10-1 Fuchinobe, Sagamihara, Kanagawa 229-8558, Japan
Bridgestone Corporation Research and Development Division, , 3-1-1 Ogawahigashi, Kodaira, Tokyo 187-8531, Japan
References (22)
Show source-provided references
1. 1999
2. Chem. Lett. · 1995 · 24 · 84110.1246/cl.1995.841 ↗
3. Thin Solid Films · 1999 · 351 · 26010.1016/S0040-6090(99)00205-9 ↗
4. Thin Solid Films · 2003 · 442 · 22710.1016/S0040-6090(03)00987-8 ↗
5. Jpn. J. Appl. Phys., Part 2 · 2003 · 42 · L152910.1143/JJAP.42.L1529 ↗
6. Jpn. J. Appl. Phys., Part 2 · 2004 · 43 · L35810.1143/JJAP.43.L358 ↗
7. Jpn. J. Appl. Phys., Part 2 · 2004 · 43 · L44210.1143/JJAP.43.L442 ↗
8. Jpn. J. Appl. Phys., Part 1 · 2002 · 41 · 81410.1143/JJAP.41.814 ↗
9. Thin Solid Films · 2003 · 445 · 20710.1016/S0040-6090(03)01152-0 ↗
10. Jpn. J. Appl. Phys., Part 1 · 2004 · 43 · 823410.1143/JJAP.43.8234 ↗
11. Thin Solid Films · 2005 · 496 · 12610.1016/j.tsf.2005.08.252 ↗
12. J. Vac. Sci. Technol. A · 1989 · 7 · 25610.1116/1.576129 ↗
13. IEICE Trans. Electron. · 2004 · 87-C · 232
14. J. Appl. Phys. · 2005 · 97 · 10N10210.1063/1.1847171 ↗
15. Surf. Coat. Technol. · 2004 · 179 · 27910.1016/S0257-8972(03)00865-X ↗
16. Sens. Actuators, A · 2007 · 133 · 25010.1016/j.sna.2006.03.027 ↗
17. J. Vac. Sci. Technol. A · 2003 · 22 · 169710.1116/1.1723289 ↗
18. J. Vac. Sci. Technol. A · 2006 · 24 · 152410.1116/1.2180273 ↗
19. J. Appl. Phys. · 1988 · 63 · 88710.1063/1.340030 ↗
20. Thin Solid Films · 2000 · 360 · 12210.1016/S0040-6090(99)00938-4 ↗
21. Phys. Rev. B · 1984 · 30 · 362510.1103/PhysRevB.30.3625 ↗
22. Thin Solid Films · 2001 · 392 · 33810.1016/S0040-6090(01)01054-9 ↗