journal article·1997-11-01

Mass and energy measurements of the species responsible for cBN growth in rf bias sputter conditions

Osamu Tsuda, Yoshinao Tatebayashi, Yukiko Yamada-Takamura, Toyonobu Yoshida

Publisher page

Abstract

Mass and energy measurements of ions and neutrals impinging on a substrate surface were performed during radio frequency (rf) bias sputter deposition of cubic boron nitride (cBN) thin films in a pure Ar discharge. The sampling system was rf driven to measure the correct energy of ions impinging to the rf driven substrate. The ion energy distributions showed asymmetric bimodal shapes and the energy spreads varied with the masses of ions and the negative substrate bias voltage (Vs). Ar+ was the most dominant ion, and the average energy and energy spread changed with Vs from 90 to 310 eV and from 40 to 140 eV, respectively. The flux ratio of Ar+ to B (Φi/ΦB) increased from 1.0 to 2.3 with a decrease in the target power input. cBN could be deposited above a threshold of the total momentum transfer per depositing boron atoms; 138 (eV amu)1/2, which is comparable to the values reported in the ion beam assisted depositions. Therefore, argon ions with an energy of 135 to 380 eV are considered to be equally contributory for cBN formation. Moreover, nucleation of cBN depends on Φi/ΦB, namely, the flux ratio of ion to boron, and requires accumulation of a certain surface state caused by ion bombardment effects, such as defects generation or densification.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Metallurgy and Materials Science, Graduate School and Faculty of Engineering, The University of Tokyo 7-3-1 Hongo, Bunkyo-ku, Tokyo, 113, Japan

References (19)

Show source-provided references
1. J. Appl. Phys. · 1992 · 72 · 50410.1063/1.351881 ↗
2. J. Mater. Res. · 1994 · 9 · 292510.1557/JMR.1994.2925 ↗
3. Diamond Relat. Mater. · 1996 · 5 · 50110.1016/0925-9635(96)80068-9 ↗
4. Diamond Relat. Mater. · 1995 · 4 · 27210.1016/0925-9635(94)05303-0 ↗
5. J. Vac. Sci. Technol. A · 1996 · 14 · 310010.1116/1.580178 ↗
6. Phys. Rev. · 1968 · 168 · 10710.1103/PhysRev.168.107 ↗
7. J. Phys. Soc. Jpn. · 1970 · 29 · 18710.1143/JPSJ.29.187 ↗
8. J. Appl. Phys. · 1985 · 58 · 402410.1063/1.335580 ↗
9. J. Appl. Phys. · 1988 · 63 · 224110.1063/1.341062 ↗
10. J. Appl. Phys. · 1991 · 69 · 292310.1063/1.348602 ↗
11. J. Appl. Phys. · 1991 · 70 · 8210.1063/1.350247 ↗
12. Diamond Relat. Mater. · 1995 · 4 · 28810.1016/0925-9635(94)05244-1 ↗
13. Diamond Relat. Mater. · 1996 · 5 · 54810.1016/0925-9635(96)80077-X ↗
14. J. Vac. Sci. Technol. A · 1993 · 13 · 2843
15. J. Vac. Sci. Technol. A · 1990 · 8 · 127710.1116/1.576911 ↗
16. J. Vac. Sci. Technol. A · 1992 · 10 · 330010.1116/1.577815 ↗
17. Thin Solid Films · 1997 · 295 · 13710.1016/S0040-6090(96)09285-1 ↗
18. Nucl. Instrum. Methods Phys. Res. B · 1995 · 106 · 9010.1016/0168-583X(95)00684-2 ↗
19. Appl. Phys. Lett. · 1997 · 70 · 94610.1063/1.118449 ↗