journal article·2014-05-01

Microstructure of surface cerium hydride growth sites

Martin Brierley, John Knowles, Neil Montgomery, Michael Preuss

Publisher page

Abstract

Samples of cerium were exposed to hydrogen under controlled conditions causing cerium hydride sites to nucleate and grow on the surface. The hydriding rate was measured in situ, and the hydrides were characterised using secondary ion mass spectrometry, scanning electron microscopy, and optical microscopy. The results show that the hydriding rate proceeded more quickly than earlier studies. Characterisation confirmed that the hydrogen is confined to the sites. The morphology of the hydrides was confirmed to be oblate, and stressed material was observed surrounding the hydride, in a number of cases lathlike features were observed surrounding the hydride sites laterally with cracking in the surface oxide above them. It is proposed that during growth the increased lattice parameter of the CeH2 induces a lateral compressive stress around the hydride, which relieves by the ca. 16% volume collapse of the γ-Ce to α-Ce pressure induced phase transition. Cracking of the surface oxide above the laths reduces the diffusion barrier to hydrogen reaching the metal/oxide interface surrounding the hydride site and contributes to the anisotropic growth of the hydrides.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Catalytic Processes in Materials Science · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Atomic Weapons Establishment , Aldermaston, Berkshire, RG7 4PR, United Kingdom and , Manchester, M13 9PL, United Kingdom

The School of Materials, University of Manchester , Aldermaston, Berkshire, RG7 4PR, United Kingdom and , Manchester, M13 9PL, United Kingdom

Atomic Weapons Establishment , Aldermaston, Berkshire, RG7 4PR, United Kingdom

The School of Materials, University of Manchester , Manchester, M13 9PL, United Kingdom

References (27)

Show source-provided references
1. Mater. Sci. · 2000 · 36 · 48110.1023/A:1011385317508 ↗
2. 1968
3. J. Nucl. Mater. · 1994 · 209 · 11310.1016/0022-3115(94)90253-4 ↗
4. Safe handling and storage of plutonium
5. Los Alamos Sci. · 2000 · 26 · 252
6. Int. J. Hydrogen Energy · 2006 · 31 · 31310.1016/j.ijhydene.2005.04.042 ↗
7. J. Phys. Chem. · 1964 · 68 · 256910.1021/j100791a030 ↗
8. Zeitschrift für anorganische und allgemeine Chemie · 1968 · 363 · 10510.1002/zaac.19683630112 ↗
9. J. Alloys Compd. · 2007 · 446–447 · 56710.1016/j.jallcom.2007.01.037 ↗
10. J. Alloys Compd. · 1993 · 191 · 9110.1016/0925-8388(93)90277-T ↗
11. J. Alloys Compd. · 1995 · 231 · 36810.1016/0925-8388(95)01849-2 ↗
12. J. Phase Equilibria · 1997 · 18 · 6310.1007/BF02646759 ↗
13. Int. J. Hydrogen Energy · 1999 · 24 · 86110.1016/S0360-3199(98)00160-8 ↗
14. J. Less-Common Met. · 1987 · 131 · 1310.1016/0022-5088(87)90496-6 ↗
15. J. Less-Common Met. · 1969 · 19 · 31510.1016/0022-5088(69)90177-5 ↗
16. Catal. Today · 2003 · 85 · 7910.1016/S0920-5861(03)00377-8 ↗
17. Surf. Sci. · 1998 · 409 · 30710.1016/S0039-6028(98)00257-X ↗
18. Philos. Mag. · 2007 · 87 · 17710.1080/14786430600919294 ↗
19. J. Alloys Compd. · 2004 · 365 · 13810.1016/S0925-8388(03)00647-9 ↗
20. J. Less-Common Met. · 1984 · 102 · 31110.1016/0022-5088(84)90326-6 ↗
21. Corros. Sci. · 2013 · 77 · 3110.1016/j.corsci.2013.07.020 ↗
22. Russ. Chem. Rev. · 1960 · 29 · 2810.1070/RC1960v029n01ABEH001216 ↗
23. J. Phys. Chem. · 1955 · 59 · 122210.1021/j150534a009 ↗
24. Ceram. Trans. · 2004 · 156 · 49
25. J. Mater. Sci. Lett. · 2001 · 20 · 21310.1023/A:1006730230387 ↗
26. Physica B+C · 1985 · 133 · 12910.1016/0378-4363(85)90406-1 ↗
27. See supplementary material at http://dx.doi.org/10.1116/1.4867475 for cracking in the surface oxide on the cerium occurs over the α-Ce laths (darker phase), providing a gas path to fresh cerium metal (Image 22) and a cerium hydride growth site with an intact oxide sectioned serially using an argon ion beam (accelerating voltage 10 kV, ion current 500 μA, normal incidence). The original metallic microstructure can be made out within the reoxidized hydride, indicating that the hydriding and subsequent reoxidation processes do not significantly alter the grain boundary microstructure (Site 5_r_avg).