Effect of AC target power on AlN film quality
Source abstract
Abstract
The influence of alternating current (AC) target power on film stress, roughness, and x-ray diffraction rocking curve full width half maximum (FWHM) was examined for AlN films deposited using S-gun magnetron sputtering on insulative substrates consisting of Si wafers with 575 nm thermal oxide. As the AC target power was increased from 5 to 8 kW, the deposition rate increased from 9.3 to 15.9 A/s, film stress decreased from 81 to −170 MPa, and the rocking curve FWHM increased from 0.98 to 1.03°. AlN film behavior is observed to change with target life; films deposited at 200 kWh target life were approximately 40 MPa more compressive and had 0.02° degree higher rocking curve FWHM values than films deposited at 130 kWh. AlN films deposited in two depositions were compared with films deposited in a single deposition, in order to better characterize the growth behavior and properties of AlN films deposited on an existing AlN film, which is not well understood. Two deposition films, when compared with single deposition films, showed no variation in residual stress trends or grain size behavior, but the average film roughness increased from 0.7 to 1.4 nm and rocking curve FWHM values increased by more than 0.25°.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Acoustic Wave Resonator Technologies · GaN-based semiconductor devices and materials · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
University of Michigan Department of Mechanical Engineering, , 2026 GG Brown—2350 Hayward St., Ann Arbor, Michigan 48109
References (31)
Show source-provided references
1. IEEE Trans. Ultrason. Ferrelectr. Freq. Control · 2010 · 57 · 3810.1109/TUFFC.2010.1376 ↗
2. IEEE Trans. Ultrason. Ferrelectr. Freq. Control · 2012 · 59 · 227010.1109/TUFFC.2012.2452 ↗
3. Mater. Res. Bull. · 2012 · 37 · 105110.1557/mrs.2012.268 ↗
4. J Microelectromech. Syst. · 2012 · 21 · 40610.1109/JMEMS.2011.2174419 ↗
5. R. Littrell, “High performance piezoelectric MEMS microphones,” Ph.D. thesis, University of Michigan, Ann Arbor (2010).
6. J. Vac. Sci. Technol. A · 2004 · 22 · 36110.1116/1.1649343 ↗
7. J. Appl. Phys. · 2001 · 89 · 638910.1063/1.1359162 ↗
8. IEEE Trans. Ultrason. Ferrelectr. Freq. Control · 2002 · 411
9. Mater. Res. Bull. · 2010 · 45 · 103910.1016/j.materresbull.2010.05.035 ↗
10. Mater. Chem. Phys. · 2003 · 79 · 14310.1016/S0254-0584(02)00252-3 ↗
11. J. Vac. Sci. Technol. A · 2009 · 27 · 41710.1116/1.3089242 ↗
12. J. Appl. Phys. · 2003 · 94 · 149510.1063/1.1587267 ↗
13. Sens. Actuators A · 2004 · 115 · 50110.1016/j.sna.2004.03.053 ↗
14. J. Vac. Sci. Technol. A · 1989 · 7 · 225210.1116/1.575923 ↗
15. Thin Solid Films · 2014 · 550 · 26410.1016/j.tsf.2013.11.073 ↗
16. Vacuum · 2010 · 2 · 12010.1016/j.vacuum.2010.04.012 ↗
17. Surf. Coat. Technol. · 2009 · 204 · 84010.1016/j.surfcoat.2009.08.007 ↗
18. J. Vac. Sci. Technol. A · 2011 · 29 · 02101410.1116/1.3554718 ↗
19. IEEE Trans. Ultrason. Ferrelectr. Freq. Control
20. J. Vac. Sci. Technol. A · 2006 · 24 · 94610.1116/1.2201042 ↗
21. J. Vac. Sci. Technol. A · 2012 · 30 · 05150110.1116/1.4732129 ↗
22. IEEE Trans. Ultrason. Ferrelectr. Freq. Control · 2003 · 2 · 2028
23. Critical Rev. Sol. State Mater. Sci. · 1992 · 17 · 54710.1080/10408439208244586 ↗
24. Vacuum · 2000 · 59 · 80610.1016/S0042-207X(00)00351-1 ↗
25. J. Mater. Res. · 2003 · 18 · 42310.1557/JMR.2003.0054 ↗
26. Microelectron. Eng. · 2011 · 88 · 80210.1016/j.mee.2010.06.045 ↗
27. McGuire · 1988
28. J. Vac. Sci. Technol. A · 1986 · 4 · 305910.1116/1.573628 ↗
29. J. Vac. Sci. Technol. A · 2010 · 28 · 39010.1116/1.3359588 ↗
30. Sens. Actuators A · 2007 · 136 · 63810.1016/j.sna.2006.12.003 ↗
31. J. Micromech. Microeng. · 2008 · 18 · 110.1088/0960-1317/18/10/105011 ↗