Chemical reactions at CdS heterojunctions with CuInSe2
Source abstract
Abstract
The stability of the CdS/CuInSe2 (CIS) heterojunction is critical to understanding the projected lifetime of CIS devices and the effect of processing conditions on the nanoscale chemistry of the heterojunction. This article reports the results of annealing heterojunctions between CdS deposited by chemical bath deposition and single crystal and polycrystalline CIS films between 200 and 500 °C for 10 to 150 min. No atomic movement was observed by secondary ion mass spectrometry at temperatures of 300 °C and below. At 400 °C even for the shortest time studied, Cu and In were found throughout the region initially consisting of CdS only and Cd was found to have moved into the CIS. In the polycrystal, annealing at 500 °C resulted in movement of Cd throughout the CIS layer. No time dependence was observed in the 400 and 500 °C anneals indicating that a reaction had occurred forming a compound that was in thermodynamic equilibrium with the remaining CIS. Diffusion turns on rapidly between 300 and 400 °C, indicating a high activation energy for atomic movement (∼2.4 eV). The onset of diffusion is consistent with the onset of Cu diffusion in CIS.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, University of Illinois , 1304 West Green Street, Urbana, Illinois 61801
References (20)
Show source-provided references
1. Q2 2010 performance summary, business update, and market outlook
2. Prog. Photovoltaics · 2011 · 19 · 89410.1002/pip.1078 ↗
3. Prog. Photovoltaics · 2008 · 16 · 23510.1002/pip.822 ↗
4. J. Appl. Phys. · 1999 · 86 · 605210.1063/1.371653 ↗
5. J. Appl. Phys. · 2003 · 93 · 938010.1063/1.1570500 ↗
6. J. Appl. Phys. · 2010 · 108 · 11490810.1063/1.3512966 ↗
7. Thin Solid Films · 2000 · 361 · 34610.1016/S0040-6090(99)00767-1 ↗
8. Appl. Phys. Lett. · 1999 · 74 · 145110.1063/1.123578 ↗
9. Junction formation in CuInSe2 based thin film devices
10. Sol. Cells · 1991 · 30 · 14310.1016/0379-6787(91)90047-S ↗
11. Nano Lett. · 2007 · 7 · 373410.1021/nl0721463 ↗
12. 2012 · 001970
13. AIP Conf. Proc. · 1999 · 462 · 12610.1063/1.57894 ↗
14. J. Vac. Sci. Technol. A · 1989 · 7 · 83710.1116/1.575851 ↗
15. Ternary compound thin film solar cells
16. Semicond. Sci. Technol. · 1997 · 12 · 96610.1088/0268-1242/12/8/006 ↗
17. J. Phys. Chem. B · 2000 · 104 · 484910.1021/jp993143k ↗
18. 1988 · 1505
19. Thin Solid Films · 2002 · 403–404 · 20410.1016/S0040-6090(01)01538-3 ↗
20. 1971