journal article·2009-07-01

Thermal stability and tribological properties of CrZr–Si–N films synthesized by closed field unbalanced magnetron sputtering

Sang Yul Lee, Young Su Kim, Gwang Seok Kim

Publisher page

Abstract

In this work, CrZr–Si–N films with various Si contents (⩽6.4at.%) were synthesized by closed field unbalanced magnetron sputtering with vertical magnetron sources. The characteristics such as hardness, surface morphology, and friction coefficient of the films as a function of the Si content after annealing up to 500°C in air were evaluated. Results revealed that the as-deposited films showed very similar characteristics irrespective of the Si content. However, after annealing at 500°C, the film characteristics showed a strong dependency upon the Si content. After annealing at 500°C, the hardness of the Cr39.4Zr12.3N48.3 film decreased significantly to approximately 24GPa and the surface roughness value increased approximately 3.5 times more than that of the as-deposited film. The Cr34.6Zr10.6–Si6.4–N48.4 film, however, was observed to have a hardness of approximately 30GPa, which is close to that of the as-deposited film, 32GPa. In addition, as the wear test temperature increased from room temperature to 500°C, the average friction coefficient of the Cr39.4Zr12.3N48.3 film increased significantly from approximately 0.23 to 0.81, but the average friction coefficient of the Cr34.6Zr10.6–Si6.4–N48.4 film was not changed extensively, measuring approximately 0.43. These results could be attributed to the improvement of the thermal stability by adding Si into the Cr–Zr–N films.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Korea Aerospace University Department of Materials Engineering, , Hangkongdae-Gil 100, KoYang-Si, KyungKi-Do 412-791, South Korea

References (20)

Show source-provided references
1. Mater. Sci. Eng., A · 1991 · 140 · 62510.1016/0921-5093(91)90487-8 ↗
2. Surf. Coat. Technol. · 1996 · 86–87 · 19210.1016/S0257-8972(96)02949-0 ↗
3. Thin Solid Films · 1998 · 332 · 24010.1016/S0040-6090(98)00992-4 ↗
4. Surf. Coat. Technol. · 2004 · 177–178 · 62710.1016/S0257-8972(03)00937-X ↗
5. Surf. Coat. Technol. · 2004 · 180–181 · 57010.1016/j.surfcoat.2003.10.121 ↗
6. Wear · 1998 · 257 · 90110.1016/j.wear.2004.05.007 ↗
7. Surf. Coat. Technol. · 2005 · 200 · 166910.1016/j.surfcoat.2005.08.101 ↗
8. Surf. Coat. Technol. · 2006 · 200 · 341110.1016/j.surfcoat.2005.02.169 ↗
9. Surf. Coat. Technol. · 2008 · 202 · 552110.1016/j.surfcoat.2008.06.101 ↗
10. Thin Solid Films · 1995 · 268 · 6410.1016/0040-6090(95)06695-0 ↗
11. Surf. Coat. Technol. · 2006 · 200 · 388610.1016/j.surfcoat.2004.12.004 ↗
12. Surf. Coat. Technol. · 2000 · 123 · 110.1016/S0257-8972(99)00395-3 ↗
13. Surf. Coat. Technol. · 2006 · 201 · 336810.1016/j.surfcoat.2006.07.206 ↗
14. Surf. Coat. Technol. · 2006 · 201 · 189410.1016/j.surfcoat.2005.12.046 ↗
15. Surf. Coat. Technol. · 1998 · 108–109 · 24110.1016/S0257-8972(98)00560-X ↗
16. J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
17. Surf. Coat. Technol. · 2008 · 102 · 397510.1016/j.surfcoat.2008.02.014 ↗
18. Surf. Coat. Technol. · 2008 · 142–144 · 954
19. Surf. Coat. Technol. · 2000 · 132 · 163810.1016/S0257-8972(00)00914-2 ↗
20. Appl. Surf. Sci. · 2004 · 229 · 13210.1016/j.apsusc.2004.01.048 ↗