Electrical behavior of atomic layer deposited high quality SiO2 gate dielectric
This record is marked as retracted by the source. Review the publisher’s notice before using its findings.
Source abstract
Abstract
Comprehensive and systematic electrical studies were performed on fabrication of high quality SiO2 thin films MOS capacitor using the robust, novel, and simple atomic layer deposition (ALD) technique using highly reactive ozone and tris (dimethylamino) silane (TDMAS) precursors. Ideal capacitance–voltage curve exhibits a very small frequency dispersion and hysteresis behavior of the SiO2 MOS capacitor grown at 1 s TDMAS pulse, suggesting excellent interfacial quality and purity of the film as probed using x-ray photoelectron studies. The flat-band voltage of the device shifted from negative toward positive voltage axis with increase of TDMAS pulses from 0.2 to 2 s. Based on an equivalent oxide thickness point of view, all SiO2 films have gate leakage current density of (5.18 × 10−8 A/cm2) as well as high dielectric break down fields of more than (∼10 MV/cm), which is better and comparable to that of thermally grown SiO2 at temperatures above 800 °C. These appealing electrical properties of ALD grown SiO2 thin films enable its potential applications such as high-quality gate insulators for thin film MOS transistors, as well as insulators for sensor and nanostructures on nonsilicon substrates. At the request of the authors, this article is being retracted effective 27 December 2014.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · Advancements in Semiconductor Devices and Circuit Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Center for Materials Research, Norfolk State University , 700 Park Ave., Norfolk, Virginia 23504
References (29)
Show source-provided references
1. P. Shekhar , L.Ming-Ren, and X.Qi, U.S. patent 6165902 (26 December 2000).
2. C. Pin-Shyne , U.S. patent 7244641 (17 July 2007).
3. 2000
4. ACS Appl. Mater. Interfaces · 2011 · 3 · 163310.1021/am200176j ↗
5. Mater. Res. Bull. · 2012 · 47 · 300410.1016/j.materresbull.2012.04.093 ↗
6. ECS Solid State Lett. · 2013 · 2 · P9110.1149/2.005310ssl ↗
7. Microelectron. Reliab. · 2002 · 42 · 182310.1016/S0026-2714(02)00095-1 ↗
8. Solid State Phenom. · 2007 · 124–126 · 24710.4028/www.scientific.net/SSP.124-126.247 ↗
9. J. Phys. Chem. C · 2009 · 113 · 824910.1021/jp806638e ↗
10. Electrochem. Solid-State Lett. · 2007 · 10 · G8010.1149/1.2763959 ↗
11. J. Phys. Chem. C · 2009 · 113 · 973110.1021/jp900119b ↗
12. ECS J. Solid State Sci. Technol. · 2013 · 2 · N22810.1149/2.001312jss ↗
13. J. Appl. Phys. · 2005 · 97 · 12130110.1063/1.1940727 ↗
14. Interface - Electrochem. Soc. · 2011 · 20 · 33
15. 2011
16. IEEE Electron. Device Lett. · 1997 · 18 · 20910.1109/55.568766 ↗
17. Appl. Phys. Lett. · 1996 · 69 · 272810.1063/1.117692 ↗
18. IEEE Trans. Electron. Devices · 1996 · 43 · 123310.1109/16.506774 ↗
19. IEEE Trans. Electron. Devices · 2004 · 51 · 50010.1109/TED.2004.823326 ↗
20. Appl. Phys. Lett. · 2008 · 92 · 19350410.1063/1.2928227 ↗
21. J. Electrochem. Soc. · 1972 · 119 · 59110.1149/1.2404268 ↗
22. 1983 · 184
23. J. Electrochem. Soc. · 1992 · 139 · 260410.1149/1.2221272 ↗
24. Appl. Phys. Lett. · 1998 · 73 · 80910.1063/1.122009 ↗
25. Chem. Vap. Deposition · 2005 · 11 · 48110.1002/cvde.200506385 ↗
26. 1922 · 46
27. J. Eur. Ceram. Soc. · 1997 · 17 · 202510.1016/S0955-2219(97)00051-4 ↗
28. J. Phys. D: Appl. Phys. · 2004 · 37 · 211210.1088/0022-3727/37/15/010 ↗
29. Surf. Interface Anal. · 2004 · 36 · 142710.1002/sia.1917 ↗