journal article·2018-01-01

Plasma-enhanced atomic layer deposition of nickel thin film using bis(1,4-diisopropyl-1,4-diazabutadiene)nickel

Jae-Min Park, Seongyoon Kim, June Hwang, Won Seok Han, Wonyong Koh, Won-Jun Lee

Publisher page

Abstract

The authors report the plasma enhanced atomic layer deposition (PEALD) of a nickel thin film using bis(1,4-diisopropyl-1,4-diazabutadiene)nickel [Ni(dpdab)2] and NH3 plasma. Ni(dpdab)2 is an oxygen-free liquid Ni precursor with a vapor pressure of 0.23 Torr at 80 °C. Ni films were deposited by alternating exposures to Ni(dpdab)2 and NH3 plasma at 125–250 °C. Ni(dpdab)2 showed the atomic layer deposition (ALD) process window between 125 and 150 °C with the ALD growth of ∼2 Å/cycle. The growth rate increased significantly above 200 °C, probably due to the thermal decomposition of the Ni precursor. The resistivity of the ALD thin film decreased with increasing radio-frequency (RF) power, and lower resistivities with high RF powers are due to the lower carbon concentration and larger grain size. The minimum resistivity of the PEALD film at 150 °C in the ALD process window was 146 μΩ cm, which is significantly higher than bulk Ni resistivity (7.0 μΩ cm) mainly due to the nitrogen content (∼13%) in the as-deposited film. For a lower nitrogen concentration, the PEALD film was annealed at 400 °C under 1 Torr of H2 for 30 min, resulting in the reduction of resistivity from 146 to 13.3 μΩ cm and removal of nitrogen impurities.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Nanotechnology and Advanced Materials Engineering, Sejong University , Seoul 05006, Republic of Korea

R&D Center, UP Chemical Co. Ltd. , Pyeongtaek-si, Gyeonggi-do 17749, Republic of Korea

Funding

UP Chemical Co.,Ltd.

References (29)

Show source-provided references
1. 2000
2. Microelectron. Eng. · 2003 · 70 · 15810.1016/S0167-9317(03)00370-8 ↗
3. Appl. Phys. Lett. · 1985 · 47 · 52710.1063/1.96115 ↗
4. J. Electrochem. Soc. · 1993 · 140 · 368910.1149/1.2221151 ↗
5. Appl. Phys. Lett. · 1995 · 67 · 230810.1063/1.115135 ↗
6. Nucl. Instrum. Methods Phys. Res., Sect. B · 2002 · 186 · 6110.1016/S0168-583X(01)00946-6 ↗
7. Curr. Appl. Phys. · 2010 · 10 · 4110.1016/j.cap.2009.04.011 ↗
8. 2004
9. Microelectron. Eng. · 2002 · 60 · 15710.1016/S0167-9317(01)00684-0 ↗
10. Thin Solid Films · 2007 · 515 · 824610.1016/j.tsf.2007.02.051 ↗
11. Mater. Sci. Eng. R · 1996 · 16 · 4310.1016/0927-796X(95)00186-7 ↗
12. Microelectron. Eng. · 2015 · 139 · 2610.1016/j.mee.2015.04.083 ↗
13. J. Phys. D: Appl. Phys. · 2006 · 39 · 280310.1088/0022-3727/39/13/025 ↗
15. Chem. Vap. Deposition · 2003 · 9 · 7310.1002/cvde.200390005 ↗
16. J. Electrochem. Soc. · 2011 · 158 · D110.1149/1.3504196 ↗
17. Electrochem. Solid-State Lett. · 2002 · 5 · C6410.1149/1.1475199 ↗
18. J. Phys. Chem. C · 2014 · 118 · 2338510.1021/jp5068318 ↗
19. Appl. Surf. Sci. · 2000 · 157 · 15110.1016/S0169-4332(99)00562-0 ↗
20. Chem. Mater. · 2010 · 22 · 306010.1021/cm903636j ↗
21. Jpn. J. Appl. Phys., Part 1 · 2006 · 45 · 297510.1143/JJAP.45.2975 ↗
22. Jpn. J. Appl. Phys. · 2010 · 49 · 05FA1110.1143/JJAP.49.05FA11 ↗
23. ACS Appl. Mater. Interfaces · 2017 · 9 · 2472210.1021/acsami.7b05571 ↗
24. Thin Solid Films · 2017 · 638 · 11410.1016/j.tsf.2017.07.041 ↗
25. W. S. Han and W. Koh, U.S. patent US20160314980 A1 (30 June 2016).
26. Appl. Phys. Lett. · 2015 · 107 · 01410210.1063/1.4926366 ↗
27. Phys. Rev. B · 2009 · 79 · 15544310.1103/PhysRevB.79.155443 ↗
28. Chem. Vap. Deposition · 2006 · 12 · 43510.1002/cvde.200606485 ↗
29. Thin Solid Films · 2014 · 556 · 43410.1016/j.tsf.2014.01.034 ↗