Detection of charge carrier confinement into mobile ionic defects in nanoporous dielectric films for advanced interconnects
Source abstract
Abstract
Reliability and robustness of low-k materials for advanced interconnects has become one of the major challenges for the continuous down-scaling of silicon semiconductor devices. Metal catalyzed time dependent breakdown is a major force preventing integration of sub-32 nm process technology nodes. Here, the authors demonstrate that ions can behave as trapping points for charge carriers. A mechanism for describing trapping of charge carriers into mobile ions under bias and temperature stress is presented. Charge carrier confinement into ionic center was found to be dominated by ionic transport. After extended bias and temperature stress, the magnitude of charge trapping into ionic centers decreased. Simulations suggest that built-in fields could reduce the effect of externally applied fields in directing ionic drift, therefore inhibiting the trapping mechanism. This work depicts the dual role of ionic species when catalyzing dielectric failure (mobile defect and local field distortion).
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Ferroelectric and Negative Capacitance Devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Howard P. Isermann Department of Chemical and Biological Engineering , Troy, New York 12180
Rensselaer Polytechnic Institute Department of Physics, , Troy, New York 12180
IBM T.J. Watson Research Center , Yorktown Heights, New York 10598
Columbia University Department of Physics and Electrical Engineering, , New York, New York 10027
University at Albany's College of Nanoscale Science and Engineering , Albany, New York 12203
References (23)
Show source-provided references
1. Science · 2001 · 293 · 204410.1126/science.293.5537.2044 ↗
2. Proc. IEEE · 2013 · 101 · 249810.1109/JPROC.2013.2252317 ↗
3. APL Mater. · 2013 · 1 · 04070110.1063/1.4822437 ↗
4. IEEE Trans. Electron Devices · 2013 · 60 · 37410.1109/TED.2012.2224663 ↗
5. 2011 · 200
6. Science · 2013 · 339 · 51210.1126/science.339.6119.512 ↗
7. Trends Cognit. Sci. · 2012 · 16 · 29210.1016/j.tics.2012.04.005 ↗
8. Appl. Phys. Rev. · 2014 · 1 · 01130610.1063/1.4861876 ↗
9. J. Appl. Phys. · 2013 · 113 · 04110110.1063/1.4765297 ↗
10. J. Appl. Phys. · 2003 · 93 · 879310.1063/1.1567460 ↗
11. 2012 · BD.1.1
12. J. Appl. Phys. · 2009 · 105 · 04490810.1063/1.3073989 ↗
13. APS March Meet. Bull. · 2013 · 58 · 23004
14. Microelectron. Reliab. · 2012 · 52 · 175310.1016/j.microrel.2012.06.007 ↗
15. Appl. Phys. Lett. · 2013 · 102 · 02290810.1063/1.4776735 ↗
16. J. Appl. Phys. · 1985 · 58 · 83110.1063/1.336152 ↗
17. IEEE Trans. Electron Devices · 2012 · 59 · 174510.1109/TED.2012.2190074 ↗
18. J. Appl. Phys. · 2013 · 113 · 03410410.1063/1.4775798 ↗
19. 2009 · 141
20. ECS Trans. · 2012 · 41 · 310.1149/1.4717497 ↗
21. 2012 · 3A-3
22. Microelectron. Reliab. · 2014 · 54 · 52910.1016/j.microrel.2013.12.020 ↗
23. 2010 · 549