journal article·2023-09-01

Large-area deposition of protective (Ti,Al)N coatings onto polycarbonate

Lena Patterer, Sabrina Kollmann, Teresa de los Arcos, Leonie Jende, Soheil Karimi Aghda, Damian M. Holzapfel, Sameer A. Salman, Stanislav Mráz, Guido Grundmeier, Jochen M. Schneider

Publisher page

Abstract

Polycarbonate (PC) and protective (Ti,Al)N coatings exhibit extremely different material properties, specifically crystal structure, thermal stability, and elastic and plastic behavior, as well as thermal expansion coefficients. These differences present formidable challenges for the deposition process development as low-temperature synthesis routes have to be explored to avoid a thermal overload of the polymer substrate. Here, a large-area sputtering process is developed to address the challenges by systematically adjusting target peak power density and duty cycle. Adhering (Ti,Al)N coatings with a critical residual tensile stress of 2.2 ± 0.2 GPa are obtained in the pulsed direct current magnetron sputtering range, whereas depositions at higher target peak power densities, realized by high power pulsed magnetron sputtering, lead to stress-induced adhesive and/or cohesive failure. The stress-optimized (Ti,Al)N coatings deposited onto PC with a target peak power density of 0.036 kW cm−2 and a duty cycle of 5.3% were investigated by the cross-cut test, confirming adhesion. By investigating the bond formation at the PC|(Ti,Al)N interface, mostly interfacial CNx bonds and a small fraction of (C−O)−(Ti,Al) bonds are identified by x-ray photoelectron spectroscopy, indicating reactions at the hydrocarbon and the carbonate groups during deposition. Nanoindentation reveals an elastic modulus of 296 ± 18 GPa for the (Ti,Al)N coating, while a Ti–Al–O layer is formed during electrochemical impedance spectroscopy in a borate buffer solution, indicating protective passivation. This work demonstrates that the challenge posed by the extremely different material properties at the interface of soft polymer substrates and hard coatings can be addressed by the systematical variation in the pulsing parameters to reduce the residual film stress.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Chemistry, RWTH Aachen University 1 , Kopernikusstr. 10, Aachen 52074, Germany

Technical and Macromolecular Chemistry, Universität Paderborn 2 , Warburger Str. 100, Paderborn 33098, Germany

Funding

Deutsche Forschungsgemeinschaft

References (67)

Show source-provided references
1. GlobalData Plc · 2022
2. Polym. Chem. · 2020 · 11 · 483010.1039/C9PY01927H ↗
3. J. Plast. Film Sheeting · 2018 · 34 · 6010.1177/8756087917691088 ↗
4. ACS Appl. Mater. Interfaces · 2020 · 12 · 1329610.1021/acsami.9b22877 ↗
5. J. Appl. Phys. · 2006 · 99 · 10431010.1063/1.2197030 ↗
6. Met. Mater. Int. · 2016 · 22 · 53510.1007/s12540-016-5492-0 ↗
7. Mater. Res. Lett. · 2017 · 5 · 15810.1080/21663831.2016.1233914 ↗
8. J. Appl. Phys. · 1990 · 67 · 154210.1063/1.345664 ↗
9. Int. J. Refract. Met. Hard. Mater. · 2012 · 31 · 8210.1016/j.ijrmhm.2011.09.010 ↗
10. Thin Solid Films · 2010 · 518 · 597810.1016/j.tsf.2010.05.064 ↗
11. Covestro AG · 2022
12. Acta Mater. · 2023 · 250 · 11886410.1016/j.actamat.2023.118864 ↗
13. Acta Mater. · 2021 · 214 · 11700310.1016/j.actamat.2021.117003 ↗
14. J. Appl. Phys. · 2017 · 121 · 17110110.1063/1.4978350 ↗
15. Surf. Coat. Technol. · 1999 · 122 · 29010.1016/S0257-8972(99)00292-3 ↗
17. Coatings · 2019 · 9 · 2410.3390/coatings9010024 ↗
18. 2009
19. Surf. Coat. Technol. · 2016 · 294 · 21010.1016/j.surfcoat.2016.03.092 ↗
20. Thin Solid Films · 2018 · 645 · 37910.1016/j.tsf.2017.11.011 ↗
21. KSME Inter. J. · 2003 · 17 · 192810.1007/BF02982432 ↗
22. Surf. Coat. Technol. · 2007 · 201 · 559610.1016/j.surfcoat.2006.07.200 ↗
23. Surf. Coat. Technol. · 2007 · 201 · 674210.1016/j.surfcoat.2006.09.046 ↗
24. Wear · 2013 · 302 · 93710.1016/j.wear.2013.01.045 ↗
25. Surf. Coat. Technol. · 2020 · 394 · 12589010.1016/j.surfcoat.2020.125890 ↗
26. Surf. Coat. Technol. · 2018 · 349 · 85810.1016/j.surfcoat.2018.06.072 ↗
27. Acta Phys. Pol. A · 2015 · 127 · 114210.12693/APhysPolA.127.1142 ↗
28. Arch. Civ. Mech. Eng. · 2012 · 12 · 46410.1016/j.acme.2012.07.004 ↗
29. J. Appl. Phys. · 2022 · 132 · 01110110.1063/5.0086359 ↗
30. Acta Mater. · 2022 · 237 · 11816010.1016/j.actamat.2022.118160 ↗
31. Surf. Sci. Spectra · 1999 · 6 · 110.1116/1.1247900 ↗
32. Phys. Rev. B · 1972 · 5 · 470910.1103/PhysRevB.5.4709 ↗
33. Kratos Analytical Ltd.
34. J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
35. J. Phys.: Condens. Matter · 2012 · 24 · 15540110.1088/0953-8984/24/15/155401 ↗
36. J. Vac. Sci. Technol. A · 2012 · 30 · 3080110.1116/1.3691832 ↗
37. See the supplementary material online for pictures of the coatings taken immediately after deposition, the analyzed area fraction of pores at the substrate-near and surface-near regions, and XPS spectra before and after CV.
38. Metals · 2019 · 9 · 26210.3390/met9020262 ↗
39. J. Appl. Phys. · 2006 · 100 · 9490610.1063/1.2360778 ↗
40. J. Phys. D: Appl. Phys. · 2000 · 33 · R17310.1088/0022-3727/33/18/201 ↗
41. Plasma Sources Sci. Technol. · 2010 · 19 · 04501410.1088/0963-0252/19/4/045014 ↗
42. Surf. Coat. Technol. · 2010 · 205 · 59110.1016/j.surfcoat.2010.07.041 ↗
43. Surf. Coat. Technol. · 2021 · 417 · 12718010.1016/j.surfcoat.2021.127180 ↗
44. Thin Solid Films · 1999 · 338 · 30410.1016/S0040-6090(98)00975-4 ↗
45. Plasma Processes Polym. · 2015 · 12 · 41610.1002/ppap.201400172 ↗
46. IOP Conf. Ser. Mater. Sci. Eng. · 2015 · 70 · 01200110.1088/1757-899X/70/1/012001 ↗
47. Materials · 2020 · 1310.3390/ma13040989 ↗
48. J. Appl. Phys. · 1993 · 73 · 858010.1063/1.353388 ↗
49. Comput. Mater. Sci. · 2020 · 183 · 10981310.1016/j.commatsci.2020.109813 ↗
50. Surf. Coat. Technol. · 2020 · 382 · 12500710.1016/j.surfcoat.2019.125007 ↗
51. J. Vac. Sci. Technol. A · 2003 · 21 · S11710.1116/1.1601610 ↗
52. Thin Solid Films · 1998 · 317 · 2710.1016/S0040-6090(97)00503-8 ↗
53. Thin Solid Films · 2010 · 518 · 408710.1016/j.tsf.2009.10.145 ↗
54. J. Appl. Phys. · 1998 · 84 · 603410.1063/1.368913 ↗
55. Thin Solid Films · 2007 · 515 · 290310.1016/j.tsf.2006.08.031 ↗
56. Surf. Coat. Technol. · 2021 · 413 · 12707610.1016/j.surfcoat.2021.127076 ↗
57. Adv. Mater. Interfaces · 2017 · 4 · 160086110.1002/admi.201600861 ↗
58. Nanoscale Res. Lett. · 2012 · 7 · 3010.1186/1556-276X-7-30 ↗
59. Appl. Surf. Sci. · 2022 · 593 · 15336310.1016/j.apsusc.2022.153363 ↗
60. Adv. Mater. Interfaces10.1002/admi.202300215 ↗
61. Acta Mater. · 2011 · 59 · 663110.1016/j.actamat.2011.07.018 ↗
62. Int. J. Thermophys. · 2004 · 25 · 22110.1023/B:IJOT.0000022336.83719.43 ↗
63. J. Phys.: Condens. Matter · 2020 · 32 · 02590110.1088/1361-648X/ab46df ↗
64. J. Mech. Behav. Mater. · 1993 · 4 · 11910.1515/JMBM.1993.4.2.119 ↗
65. J. Appl. Phys. · 2014 · 116 · 9351510.1063/1.4894776 ↗
66. Microelectron. J. · 2004 · 35 · 59510.1016/j.mejo.2004.02.004 ↗
67. Electrochim. Acta · 2016 · 208 · 12010.1016/j.electacta.2016.05.011 ↗