Continuous emission of O− ions into a vacuum from a bare surface of yttria-stabilized zirconia at elevated temperatures
Source abstract
Abstract
Emission of oxygen negative ions O− from a bare surface of yttria-stabilized zirconia (YSZ) was studied at 925°C with a quadrupole mass spectrometer capable of detecting negative ions. The use of the mass spectrometer allowed one to identify O− ions, thereby enabling the investigation of emission stability of O− ions. Experimental results demonstrated that O− ions were emitted from the surface of YSZ continuously over 120h. Although emission rate of O− ions decreased gradually with time, the emission rate of O− ions was confirmed to be temporarily restored after intervals. It was found that time constant of decay curve of O− ions was different from that of emission current. An analysis of the decay curves indicated that the difference in the time constants would be due to emission of electrons. Further, the analysis indicated that the number of emitted electrons would decrease with time more rapidly than O− ions, suggesting that it would be attributed to a variation in surface density of chemisorbed oxygen species on emission surface.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Analytical Chemistry and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Tohoku University Institute of Multidisciplinary Research for Advanced Materials, , 2-1-1 Katahira, Aoba-ku, Sendai 980-8577, Japan
References (32)
Show source-provided references
1. Vacuum · 1990 · 41 · 166110.1016/0042-207X(90)94047-T ↗
2. Int. J. Mass Spectrom. Ion Process. · 1995 · 143 · 5110.1016/0168-1176(94)04135-T ↗
3. Jpn. J. Appl. Phys. · 1966 · 5 · 73710.1143/JJAP.5.737 ↗
4. J. Vac. Sci. Technol. B · 1995 · 13 · 163910.1116/1.587871 ↗
5. Jpn. J. Appl. Phys., Part 1 · 2000 · 39 · 132710.1143/JJAP.39.1327 ↗
6. Surf. Sci. · 1972 · 32 · 22210.1016/0039-6028(72)90130-6 ↗
7. Appl. Phys. Lett. · 1992 · 60 · 268410.1063/1.106895 ↗
8. Electron. Lett. · 1978 · 14 · 59310.1049/el:19780397 ↗
9. Nucl. Instrum. Methods Phys. Res. B · 1990 · 44 · 27810.1016/0168-583X(90)90640-G ↗
10. Nucl. Instrum. Methods Phys. Res. B · 2001 · 175–177 · 458
11. Rev. Sci. Instrum. · 1986 · 57 · 151210.1063/1.1138577 ↗
12. Nucl. Instrum. Methods Phys. Res. B · 1995 · 96 · 710.1016/0168-583X(94)00444-7 ↗
13. Rev. Sci. Instrum. · 1992 · 63 · 236810.1063/1.1142932 ↗
14. Rev. Sci. Instrum. · 1994 · 65 · 129010.1063/1.1144984 ↗
15. Nucl. Instrum. Methods Phys. Res. · 1965 · 32 · 35710.1016/0029-554X(65)90539-2 ↗
16. Nucl. Instrum. Methods Phys. Res. · 1973 · 113 · 29910.1016/0029-554X(73)90847-1 ↗
17. Rev. Sci. Instrum. · 1995 · 66 · 491110.1063/1.1146173 ↗
18. Singhal · 2002 · 185
19. J. Electrochem. Soc. · 2003 · 150 · E11710.1149/1.1536995 ↗
20. 1981
21. J. Am. Ceram. Soc. · 1964 · 47 · 12210.1111/j.1151-2916.1964.tb14368.x ↗
22. Jpn. J. Appl. Phys., Part 2 · 1997 · 36 · L23810.1143/JJAP.36.L238 ↗
23. Trans. Mater. Res. Soc. Jpn. · 2002 · 27 · 85
24. J. Catal. · 2002 · 209 · 25610.1006/jcat.2002.3541 ↗
25. Jpn. J. Appl. Phys., Part 2 · 2002 · 41 · L65710.1143/JJAP.41.L657 ↗
26. J. Catal. · 2003 · 215 · 110.1016/S0021-9517(02)00041-6 ↗
27. J. Electrochem. Soc. · 2003 · 150 · E54310.1149/1.1611495 ↗
28. J. Alloys Compd. · 2006 · 408–412 · 1127
29. Jpn. J. Appl. Phys., Part 2 · 2002 · 41 · L53010.1143/JJAP.41.L530 ↗
30. Appl. Phys. Lett. · 2002 · 80 · 425910.1063/1.1476958 ↗
31. Electrochem. Solid-State Lett. · 2002 · 5 · J1310.1149/1.1498970 ↗
32. J. Electrochem. Soc. · 2002 · 149 · A129310.1149/1.1506981 ↗