Characterization of thin ZrO2 films deposited using (ZrOi–Pr)2(thd)2 and O2 on Si(100)
Source abstract
Abstract
The properties of ZrO2 films deposited using molecular oxygen and a recently developed precursor, zirconium Zr(Oi–Pr)2(thd)2 have been investigated. The organometallic was dissolved as a 0.15 molar solution in octane and introduced into the deposition chamber using a liquid injection system. The deposition rate was insensitive to molecular oxygen flow but changed with liquid injection rate and was thermally activated in the range 390 °C–550 °C. Carbon concentrations, <0.1 at. %, the detection limit of the x-ray photoelectron spectroscopy depth profiling measurements, were obtained at the lowest deposition temperatures and deposition rates. High-resolution transmission electron microscopy showed the films to be polycrystalline as deposited, with a zirconium silicate interfacial layer. After proper annealing treatments, an equivalent oxide thickness (EOT) of around 2.3 nm has been achieved for a 5.2 nm thick film, with a leakage current two orders of magnitude lower than that of SiO2 with the same EOT. Promising capacitance–voltage characteristics were also achieved, but some improvements are required if these films are to be used as a gate insulator.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Electronic and Structural Properties of Oxides · Integrated Circuits and Semiconductor Failure Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Electronics Engineering, National Chiao-Tung University, Hsinchu 300, Taiwan, Republic of China
Institute for Microstructural Sciences, National Research Council of Canada, Ottawa, Ontario K1A OR6, Canada
Department of Electrophysics, National Chiao-Tung University, Hsinchu 300, Taiwan, Republic of China
National Chiao-Tung University, Hsinchu 300, Taiwan, Republic of China
References (9)
Show source-provided references
1. IEEE Electron Device Lett. · 1997 · 18 · 20910.1109/55.568766 ↗
2. Appl. Phys. Lett. · 1996 · 69 · 272810.1063/1.117692 ↗
3. J. Mater. Res. · 1996 · 11 · 275710.1557/JMR.1996.0350 ↗
4. J. Appl. Phys. · 2001 · 89 · 524310.1063/1.1361065 ↗
5. J. Vac. Sci. Technol. B · 2000 · 18 · 178510.1116/1.591472 ↗
6. Chem. Vap. Deposition · 1998 · 4 · 4610.1002/(SICI)1521-3862(199803)04:02<46::AID-CVDE46>3.0.CO;2-1 ↗
7. J. Appl. Phys. · 1996 · 79 · 6658
8. J. Appl. Phys. · 1993 · 74 · 478010.1063/1.355311 ↗
9. J. Appl. Phys. · 2000 · 87 · 861510.1063/1.373587 ↗