journal article·1991-03-01

Phase selective deposition of boron achieved by crystallization control

U. Jansson, M. Boman, L. C. Markert, J.-O. Carlsson, J. E. Greene

Publisher page

Abstract

The growth kinetics and phase composition of boron films deposited by chemical vapor deposition from H2/BCl3 mixtures depend strongly upon the choice of substrate material. We have demonstrated phase-selective deposition of amorphous boron (a-B) and crystalline α-rhombohedral boron (α-B) on a substrate patterned with Ti and Mo regions. a-B was obtained on Ti at growth temperatures up to 1500 K, well above the normal stability temperature of the amorphous phase, while at the same time α-B was obtained on the exposed Mo region of the substrate. The interface between the two phases remained abrupt and vertical for film growth to thicknesses >10 μm.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Semiconductor materials and interfaces · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry, Thin Film and Surface Chemistry Group, University of Uppsala, Box 531, S-751 21, Uppsala, Sweden

Department of Materials Science, Coordinated Science Laboratory and Materials Research Laboratory, University of Illinois, Urbana, Illinois 61801

References

Reference metadata was not supplied for this record.