Dependence of the electrical properties of KNO3 memory devices on fabrication and processing parameters
Source abstract
Abstract
Several fabrication and processing parameters such as deposition rate, thickness of the sample, annealing time and temperature, and electrode materials were varied in Au–KNO3 –Au thin-film ferroelectric memory devices to optimize the electrical properties of these devices. The deposition rate was varied from 2.5 to 10 nm/min in steps of 2.5 nm/min. The samples deposited at a rate of 5 nm/min yielded better electrical results compared to samples deposited at other rates. The electrical testing involved pulse testing and capacitance–voltage measurements. The switching time of these devices decreased with a decrease in the thickness of KNO3 as expected. However, the switching thresholds were sharper in the 200-nm-thick KNO3, as compared to 160- and 120-nm-thick KNO3 samples. The samples were annealed in forming gas at 6, 10, 17, 21, 24, and 44 h and no significant changes were observed in the switching time and polarization. Instead of gold electrodes, indium–tin electrodes gave better performance but they were not easily repeatable.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Ferroelectric and Piezoelectric Materials · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Electrical Engineering, Michigan Technological University, Houghton, Michigan 49931
References
Reference metadata was not supplied for this record.