Influence of residual stress and film thickness on crystallographic orientation in Al thin films deposited by bias sputtering
Source abstract
Abstract
Al thin films with various residual stress and film thickness were deposited by bias sputtering. Residual stress and relative intensity of the (200) to (111) plane of Al thin films were measured by x-ray diffraction. When film thickness is fixed at 1 μm below the residual stress of ∼80 MPa, Al thin films have a (111) orientation, but above this stress, a (100) orientation. If Al thin films are in the high residual stress of ∼145 MPa, crystallographic orientation changes to a (100) from a (111) orientation as film thickness increases to 2 μm from 1 μm. However, Al thin films with the residual stress of ∼25 MPa have a (111) orientation regardless of film thickness. Total energy for Al thin films of a (100) and a (111) orientation was calculated as a function of residual stress and film thickness. These experimental results could be explained by the minimization of the sum of strain energy and surface energy in the films.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Copper Interconnects and Reliability · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Dae-Jon 305-701, Korea
References (19)
Show source-provided references
1. Jpn. J. Appl. Phys. · 1981 · 20 · L16910.1143/JJAP.20.L169 ↗
2. J. Appl. Phys. · 1986 · 60 · 36110.1063/1.337654 ↗
3. J. Appl. Phys. · 1959 · 30 · 135910.1063/1.1735335 ↗
4. J. Vac. Sci. Technol. A · 1991 · 9 · 54710.1116/1.577406 ↗
5. J. Korean Ceram. Soc. · 1995 · 32 · 950
6. J. Phys.: Condens. Matter · 1996 · 8 · 5883
7. Thin Solid Films · 1991 · 197 · 11710.1016/0040-6090(91)90225-M ↗
8. J. Vac. Sci. Technol. A · 1993 · 11 · 297010.1116/1.578677 ↗
9. J. Appl. Phys. · 1990 · 68 · 97310.1063/1.346663 ↗
10. Thin Solid Films · 1982 · 92 · 4110.1016/0040-6090(82)90186-9 ↗
11. J. Appl. Phys. · 1977 · 48 · 392510.1063/1.324266 ↗
12. Metall. Trans. A · 1970 · 1 · 72510.1007/BF02811600 ↗
13. J. Vac. Sci. Technol. A · 1995 · 13 · 283210.1116/1.579713 ↗
14. J. Appl. Phys. · 1987 · 62 · 179610.1063/1.339559 ↗
15. CRC Crit. Rev. Solid State Mater. Sci. · 1992 · 17 · 54710.1080/10408439208244586 ↗
16. J. Appl. Phys. · 1959 · 30 · 597
17. J. Appl. Phys. · 1965 · 36 · 216910.1063/1.1714442 ↗
18. J. Appl. Phys. · 1968 · 39 · 277310.1063/1.1656671 ↗
19. J. Appl. Phys. · 1969 · 40 · 70910.1063/1.1657457 ↗