Abstract

Multilayered physical vapor deposited TiN/TaNx coatings were deposited on cemented carbide substrates using a dual target magnetron sputtering system. The coatings were investigated with respect to the influence of nitrogen partial pressure during deposition on the residual stress developed in the coatings. Furthermore, the fracture strength of the material, i.e., the magnitude of the tensile stress that the coating can support without cracking, was evaluated. It was found that, by increasing the nitrogen partial pressure, it is possible to change the stress from compressive to tensile. The highest tensile stress was about 3.6 GPa. Despite this high stress, the coating displayed no cracking. This implies that it is possible to grow TiN/TaNx multilayered coatings with high tensile fracture strength using dual magnetron sputtering and a high deposition temperature (about 680 °C).
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

AB Sandvik Coromant, SE-126 80 Stockholm, Sweden

Materials Science Division, The Ångström Laboratory, Uppsala University, Box 534, SE-751 21 Uppsala, Sweden

Thin Film Physics Division, Department of Physics, IFM, Linköping University, SE-581 83 Linköping, Sweden

References (23)

Show source-provided references
1. Surf. Coat. Technol. · 1992 · 54/55 · 17310.1016/0257-8972(92)90158-7 ↗
2. Surf. Coat. Technol. · 1991 · 46 · 26510.1016/0257-8972(91)90169-W ↗
3. Crit. Rev. Solid State Mater. Sci. · 1992 · 17 · 6
4. J. Vac. Sci. Technol. · 1986 · 4 · 610.1116/1.583354 ↗
5. Thin Solid Films · 1992 · 207 · 11710.1016/0040-6090(92)90111-N ↗
6. Thin Solid Films · 1987 · 154 · 12510.1016/0040-6090(87)90358-0 ↗
7. Phys. Status Solidi A · 1996 · 158 · 50510.1002/pssa.2211580218 ↗
8. Surf. Coat. Technol. · 1995 · 76 · 265
9. Surf. Coat. Technol. · 1995 · 77 · 265
10. J. Vac. Sci. Technol. · 1982 · 20 · 35510.1116/1.571463 ↗
11. J. Vac. Sci. Technol. · 1980 · 17 · 38010.1116/1.570394 ↗
12. Phys. Rev. B · 1990 · 41 · 10
13. J. Vac. Sci. Technol. A · 1998 · 16 · 310410.1116/1.581466 ↗
14. Wear · 1999 · 232 · 26210.1016/S0043-1648(99)00155-6 ↗
15. Surf. Coat. Technol. · 1997 · 90 · 9110.1016/S0257-8972(96)03099-X ↗
16. Surf. Eng. · 1996 · 12 · 110.1179/sur.1996.12.1.1 ↗
17. J. Vac. Sci. Technol. A · 1984 · 2 · 3
18. Vacuum · 1984 · 34 · 10
19. J. Vac. Sci. Technol. · 1979 · 18 · 2
20. Vacuum · 1990 · 41 · 4
21. Thin Solid Films · 1980 · 66 · 21710.1016/0040-6090(80)90225-4 ↗
22. CRC Crit. Rev. Solid State Mater. Sci. · 1988 · 14 · 3
23. Phys. Status Solidi A · 1990 · 230 · 2