W and WSix Ohmic contacts on p- and n-type GaN

X. A. Cao, F. Ren, S. J. Pearton, A. Zeitouny, M. Eizenberg, J. C. Zolper, C. R. Abernathy, J. Han, R. J. Shul, J. R. Lothian

Abstract

W and WSi Ohmic contacts on both p- and n-type GaN have been annealed at temperatures from 300 to 1000 °C. There is minimal reaction (⩽100 Å broadening of the metal/GaN interface) even at 1000 °C. Specific contact resistances in the 10−5 Ω cm2 range are obtained for WSix on Si-implanted GaN with a peak doping concentration of ∼5×1020 cm−3, after annealing at 950 °C. On p-GaN, leaky Schottky diode behavior is observed for W, WSix and Ni/Au contacts at room temperature, but true Ohmic characteristics are obtained at 250–300 °C, where the specific contact resistances are, typically, in the 10−2 Ω cm2 range. The best contacts for W and WSix are obtained after 700 °C annealing for periods of 30–120 s. The formation of β-W2N interfacial phases appear to be important in determining the contact quality.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: GaN-based semiconductor devices and materials · Metal and Thin Film Mechanics · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering, University of Florida, Gainesville, Florida 32611

Department of Chemical Engineering, University of Florida, Gainesville, Florida 32611

Department of Materials Engineering, Technion–Israel Institute of Technology, Haifa 32000, Israel

Office of Naval Research, Arlington, Virginia 22217

Sandia National Laboratories, Albuquerque, New Mexico 87185

Bell Laboratories, Lucent Technologies, Murray Hill, New Jersey 07974

References (24)

Show source-provided references
1. Appl. Phys. Lett. · 1994 · 64 · 168710.1063/1.111832 ↗
2. MRS Internet J. Nitride Semicond. Res. · 1997 · 2 · 4410.1557/S1092578300001708 ↗
3. J. Appl. Phys. · 1997 · 81 · 131510.1063/1.363912 ↗
4. MRS Internet J. Nitride Semicond. Res. · 1996 · 1 · 3810.1557/S1092578300002106 ↗
5. Mater. Res. Soc. Symp. Proc. · 1997 · 468 · 42110.1557/PROC-468-421 ↗
6. Mater. Res. Soc. Symp. Proc. · 1997 · 97-1 · 171
7. Jpn. J. Appl. Phys., Part 2 · 1995 · 34 · L151710.7567/JJAP.34.L1517 ↗
8. J. Mater. Res. · 1997 · 12 · 224910.1557/JMR.1997.0300 ↗
9. Appl. Phys. Lett. · 1996 · 69 · 353710.1063/1.117237 ↗
10. Mater. Res. Soc. Symp. Proc. · 1997 · 468 · 42710.1557/PROC-468-427 ↗
11. Mater. Res. Soc. Symp. Proc. · 1997 · 449 · 1091
12. Mater. Res. Soc. Symp. Proc. · 1996 · 395 · 861
13. Mater. Res. Soc. Symp. Proc. · 1996 · 395 · 819
14. Mater. Res. Soc. Symp. Proc. · 1997 · 449 · 1061
15. Solid–State Electron. · 1998 · 42 · 67710.1016/S0038-1101(98)00099-9 ↗
16. J. Electrochem. Soc. · 1997 · 144 · L27510.1149/1.1838007 ↗
17. Appl. Phys. Lett. · 1997 · 71 · 300410.1063/1.120244 ↗
18. J. Appl. Phys. · 1996 · 80 · 27810.1063/1.362816 ↗
19. MRS Bull. · 1997 · 22 · 36
20. Mater. Res. Soc. Symp. Proc. · 1997 · 468 · 5110.1557/PROC-468-51 ↗
21. Appl. Phys. Lett. · 1996 · 68 · 227310.1063/1.115882 ↗
22. Mater. Res. Soc. Symp. Proc. · 1997 · 468 · 43110.1557/PROC-468-431 ↗
23. Phys. Rev. B · 1993 · 48 · 243610.1103/PhysRevB.48.2436 ↗
24. Mater. Res. Soc. Symp. Proc. · 1996 · 395 · 843