Room temperature preparation of activated and crystallized p-type Si1−xGex thin film on glass substrate by intense, pulsed, ion beam evaporation
Source abstract
Abstract
A boron doped Si1−xGex thin film has been successfully prepared on a quartz (SiO2) glass substrate at room temperature (RT) by irradiating an intense, pulsed, ion beam on a Si–Ge–B pellet. As a result, in situ boron doped Si1−xGex thin film was found to be crystallized. In addition, by van der Pauw measurement, the resistivity, carrier density, and mobility of the thin film were observed as ρ=2.3×10−3Ωcm, n=7.2×1020cm−3, and μ=3.8cm2∕Vs, respectively. Thus, the boron doped Si1−xGex thin film was clarified to be not only crystallized but also activated without heat treatment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon Nanostructures and Photoluminescence · Thin-Film Transistor Technologies · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Extreme Energy-Density Research Institute , Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
Department of Mechanical Engineering , Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
Department of Electrical Engineering , Nagaoka University of Technology, 1603-1 Kamitomioka, Nagaoka, Niigata 940-2188, Japan
References (13)
Show source-provided references
1. J. Phys. IV · 1993 · 3 · 427
2. J. Vac. Sci. Technol. B · 1994 · 12 · 120310.1116/1.587044 ↗
3. Thin Solid Films · 1999 · 343–344 · 541
4. Thin Solid Films · 2000 · 368 · 5510.1016/S0040-6090(00)00922-6 ↗
5. Thin Solid Films · 2000 · 369 · 17110.1016/S0040-6090(00)00800-2 ↗
6. Trans. Mater. Res. Soc. Jpn. · 2003 · 28 · 429
7. Hora · 1992 · 567
8. Appl. Phys. Lett. · 1996 · 69 · 219310.1063/1.117162 ↗
9. Appl. Phys. Lett. · 2002 · 80 · 115310.1063/1.1449539 ↗
10. Mater. Chem. Phys. · 1998 · 54 · 21910.1016/S0254-0584(98)00030-3 ↗
11. Jpn. J. Appl. Phys., Part 1 · 2001 · 40 · 103510.1143/JJAP.40.1035 ↗
12. Phys. Rev. · 1958 · 112 · 154610.1103/PhysRev.112.1546 ↗
13. Enhanced Thermal Donor Formation and Oxygen Diffusion in Silicon Exposed to Atomic Hydrogen