Parametric study of sputtered Sr-deficient SrBi2Ta2O9 thin films

Sam Zhang, Yibin Li, Weidong Fei, Zhenghao Gan, Subodh Mhaisalkar, X. M. Li

Publisher page

Abstract

Sr-deficient SrBi2Ta2O9 (SBT) thin films for nonvolatile ferroelectric random access memory applications were deposited by radio-frequency magnetron sputtering on Pt∕Ta∕SiO2∕Si substrates. The effect of deposition parameters on microstructures and chemical composition were studied using x-ray diffraction (XRD), field emission scanning electron microscopy, and x-ray photoelectron spectroscopy (XPS). The composition of the films was dependent on the sputtering conditions. The undesirable pyrochlore phase could be eliminated by adjusting process pressure, target power density, and target-to-substrate distance. The evolution of microstructures at various deposition conditions was attributed to changes in the Bi∕Ta and Sr∕Ta ratios. When Sr became deficient and Bi excessive (Sr0.74Bi2.2Ta2O9+x as determined by XPS), no pyrochlore phase was detected with XRD. Under an electric field of 240kV∕cm, the Sr-deficient SBT film demonstrated a remnant polarization (2Pr) of 11.6μC∕cm2 and a coercive field (2Ec) of 96kV∕cm.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Multiferroics and related materials · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Nanyang Technological University School of Mechanical and Aerospace Engineering, , 50 Nanyang Avenue, Singapore 639798, Singapore

Harbin Institute of Technology School of Materials Science and Engineering, , 92 West Dazhi Street, Harbin 150001, People’s Republic of China

Nanyang Technological University School of Materials Science and Engineering, , 50 Nanyang Avenue, Singapore 639798, Singapore

Shanghai Institute of Ceramics State Key Laboratory of High Performance Ceramics and Superfine Microstructures, , Chinese Academy of Sciences, 1295 Ding Xi Road, Shanghai 200050, People’s Republic of China

References (32)

Show source-provided references
1. Appl. Phys. Lett. · 1995 · 66 · 23910.1063/1.113558 ↗
2. Appl. Phys. Lett. · 1999 · 74 · 148410.1063/1.123588 ↗
3. J. Phys. D · 2000 · 33 · 90610.1088/0022-3727/33/8/304 ↗
4. J. Electrochem. Soc. · 2004 · 151 · F8710.1149/1.1667522 ↗
5. Appl. Phys. Lett. · 1995 · 67 · 57210.1063/1.115173 ↗
6. J. Phys. Chem. Solids · 1962 · 23 · 66510.1016/0022-3697(62)90526-7 ↗
7. Appl. Phys. Lett. · 1999 · 74 · 190410.1063/1.123708 ↗
8. Appl. Phys. Lett. · 1996 · 69 · 171910.1063/1.118008 ↗
9. Appl. Phys. A: Mater. Sci. Process. · 2000 · 70 · 28310.1007/s003390050048 ↗
10. Appl. Phys. Lett. · 1998 · 73 · 16610.1063/1.121744 ↗
11. Appl. Phys. Lett. · 1997 · 70 · 108010.1063/1.118485 ↗
12. Appl. Phys. Lett. · 1995 · 66 · 22110.1063/1.113140 ↗
13. Nature (London) · 1995 · 374 · 62710.1038/374627a0 ↗
14. Appl. Phys. Lett. · 1996 · 69 · 383910.1063/1.117122 ↗
15. J. Mater. Res. · 2002 · 17 · 145510.1557/JMR.2002.0216 ↗
16. Appl. Phys. Lett. · 1999 · 18 · 2827
17. J. Korean Phys. Soc. · 2003 · 42 · S1117
18. Jpn. J. Appl. Phys., Part 1 · 1995 · 34 · 509610.1143/JJAP.34.5096 ↗
19. J. Appl. Phys. · 2002 · 92 · 105610.1063/1.1486031 ↗
20. Appl. Phys. Lett. · 1999 · 75 · 265010.1063/1.125107 ↗
21. Appl. Surf. Sci. · 2005 · 252 · 4910.1016/j.apsusc.2005.01.112 ↗
22. J. Mater. Res. · 1996 · 11 · 228210.1557/JMR.1996.0290 ↗
23. J. Non-Cryst. Solids · 2003 · 320 · 77
24. J. Vac. Sci. Technol. A · 1999 · 17 · 2958
25. Thin Solid Films · 2000 · 372 · 197
26. Thin Solid Films · 1991 · 59 · 199
27. J. Appl. Phys. · 1979 · 50 · 367710.1063/1.326321 ↗
28. J. Vac. Sci. Technol. · 1978 · 15 · 110.1116/1.569429 ↗
29. J. Vac. Sci. Technol. A · 1995 · 13 · 241210.1116/1.579482 ↗
30. J. Vac. Sci. Technol. A · 1986 · 4 · 40810.1116/1.573892 ↗
31. J. Vac. Sci. Technol. A · 1998 · 16 · 125810.1116/1.581270 ↗
32. Jpn. J. Appl. Phys., Part 1 · 2000 · 39 · 557310.1143/JJAP.39.5573 ↗