journal article·2020-07-01

Antioxidation protection for Ce metal by atomic layer deposition upon air exposure

Lihua Zhou, Yiwu Chen, Qiang Yang, Yingxi Zhu, Jing Zhao, Tianfu Li, Xiaoyu Zou, Jian Wang, Tinggui Yang

Publisher page

Abstract

Some extremely reactive metals like Ce, U, and Pu are easily oxidized; instead of forming a stable surface oxide layer preventing further oxidation, the oxide layer break into powders as exposed to air in few days. For nuclear mineral industry, these materials need to be in storage for 1 month or so, which need to minimize surface oxidation. To provide a novel way to storage, atomic layer deposition (ALD) of thin Al2O3 film on the Ce metal surface is demonstrated, which prevents the oxidation of Ce for 40 days with just 2 nm of Al2O3. ALD also minimizes the foreign elements of passivation materials with great uniformity for different shapes, which unveils the potential for extremely reactive metal passivation in nuclear industry.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Radioactive element chemistry and processing · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Chengdu Nuclear Engineering Design and Research Institute Co., Ltd. , 404, CNNC, 888 Tianfu Road, Tianfu District, Chengdu 732850, China

References (29)

Show source-provided references
1. J. Nucl. Mater. · 2011 · 410 · 1010.1016/j.jnucmat.2010.12.218 ↗
2. J. Alloys Compd. · 2001 · 314 · 7810.1016/S0925-8388(00)01222-6 ↗
3. J. Nucl. Mater. · 2015 · 465 · 75610.1016/j.jnucmat.2015.06.058 ↗
4. Los Alamos Sci. · 2000 · 26 · 252
5. J. Am. Ceram. Soc. · 2013 · 96 · 294310.1111/jace.12496 ↗
6. Phys. Chem. Chem. Phys. · 2016 · 18 · 2285210.1039/C6CP03543D ↗
7. Sci. Rep. · 2016 · 6 · 110.1038/s41598-016-0001-8 ↗
8. Beilstein J. Nanotechnol. · 2018 · 9 · 89010.3762/bjnano.9.83 ↗
9. Corros. Sci. · 2016 · 111 · 5210.1021/ja01125a018 ↗
10. Surf. Sci. Rep. · 2015 · 70 · 4210.1016/j.surfrep.2014.12.001 ↗
11. Mater. Today · 2014 · 17 · 23610.1016/j.mattod.2014.04.026 ↗
12. Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
13. J. Vac. Sci. Technol. A · 2015 · 33 · 02080210.1116/1.4913379 ↗
14. ACS Appl. Mater. Interfaces · 2015 · 7 · 2212110.1021/acsami.5b06891 ↗
15. Sci. Technol. Adv. Mater. · 2019 · 20 · 46510.1080/14686996.2019.1599694 ↗
16. Chem. Mater. · 2015 · 27 · 645710.1021/acs.chemmater.5b02789 ↗
17. J. Hazard. Mater. · 2019 · 378 · 12065510.1016/j.jhazmat.2019.05.048 ↗
18. J. Electron. Mater. · 2019 · 48 · 757310.1007/s11664-019-07534-7 ↗
19. AIP Adv. · 2016 · 6 · 01501610.1063/1.4941063 ↗
20. J. Vac. Sci. Technol. A · 2012 · 30 · 04080210.1116/1.4728205 ↗
21. Appl. Phys. Lett. · 2009 · 94 · 23330510.1063/1.3153123 ↗
22. J. Vac. Sci. Technol. A · 2016 · 34 · 04C10310.1116/1.4952401 ↗
23. ACS Appl. Mater. Interfaces · 2017 · 9 · 419210.1021/acsami.6b13571 ↗
24. J. Vac. Sci. Technol. A · 2019 · 37 · 06090210.1116/1.5116136 ↗
25. Sci. Rep. · 2019 · 9 · 110.1038/s41598-018-37186-2 ↗
26. Langmuir · 1996 · 12 · 179410.1021/la950002a ↗
27. Surf. Interface Anal. · 2008 · 40 · 26410.1002/sia.2686 ↗
28. Nanotechnology · 2019 · 30 · 08570310.1088/1361-6528/aae364 ↗
29. See supplementary material at http://dx.doi.org/10.1116/6.0000223 for cross section TEM images of samples with 10, 20, and 40 cycles of ALD of Al2O3 upon air exposure for 90 days.