journal article·1988-05-01

Residual hydrogen concentration levels in graphite

R. Bastasz

Publisher page

Abstract

Hydrogen concentration versus depth profiles obtained with secondary ion mass spectrometry of a high-purity graphite (POCO) indicate that unannealed POCO has a residual subsurface H level on the order of 0.4% H/C. Vacuum annealing to 910 °C for several hours reduces this level by over an order of magnitude. However, reabsorption of hydrogen containing gases during air exposure occurs in the near surface region. Prolonged air exposure brings the residual hydrogen level within 5 μm of the surface back to the levels seen in unannealed POCO samples.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ion-surface interactions and analysis · Nuclear Physics and Applications · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Sandia National Laboratories, Livermore, California 94550

References