journal article·2006-05-01

Electrical property improvements of yttrium oxide-based metal-insulator-metal capacitors

C. Durand, C. Vallée, C. Dubourdieu, M. Kahn, M. Derivaz, S. Blonkowski, D. Jalabert, P. Hollinger, Q. Fang, I. W. Boyd

Publisher page

Abstract

We investigate the effects of the thickness reduction and specific postannealing treatments in order to improve the electrical properties of yttrium oxide-based metal-insulator-metal (MIM) capacitors. The films were grown on Si∕TiSi2∕TiN substrates at 350°C by a low temperature process (pulsed liquid injection plasma-enhanced metal organic chemical vapor deposition). Although the thickness reduction leads to an increase of the capacitance density, the other electrical characteristics (the voltage linearity, the leakage currents, and the voltage breakdown) are seriously deteriorated due to the augmentation of the electric field. Low thermal budget annealing posttreatments (⩽450°C) were carried out in a gas flux (Ar, O2, and H2) and under an ultraviolet (UV) radiation (O2 and N2). We demonstrate that the UV-O2 annealing treatment is particularly efficient in improving the voltage linearity, the leakage currents, and the electric field breakdown. The improved electrical properties after the UV-O2 annealing can be related to chemical modifications (organic content reduction and oxygen content increase). The voltage linearity improvement is most likely due to the presence of a residual oxidized silicon ultrathin layer on the top surface of the yttrium oxide films. Thus, a UV-O2 annealing is an effective postdeposition treatment that is compatible with the low thermal budget, which is required for MIM applications.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Dielectric materials and actuators

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratoire des Technologies de la Microélectronique (LTM) , UMR CNRS 5129, 17 Avenue des Martyrs, 38054 Grenoble Cedex 9, France

Laboratoire des Matériaux et du Génie Physique (LMGP) , UMR CNRS 5628, ENSPG, Boîte Postale 46, 38402 St. Martin d’Hères, France

ST-Microelectronics , 850 Rue Jean Monnet, 38926 Crolles Cedex, France

CEA Grenoble , 17 Avenue des Martyrs, 38054 Grenoble Cedex 9, France

University College London Department of Electronic and Electrical Engineering and London Centre for Nanotechnology, , Torrington Place, London WC1E 7JE, United Kingdom and London Centre for Nanotechnology, , Torrington Place, London WC1E 7JE, United Kingdom

References (39)

Show source-provided references
1. 2000 · 106
2. 1999 · 245
3. Tech. Dig. - Int. Electron Devices Meet. · 2000 · 153
4. IEEE Electron Device Lett. · 2001 · 22 · 23010.1109/55.919238 ↗
5. J. Appl. Phys. · 2001 · 90 · 150110.1063/1.1381043 ↗
6. J. Appl. Phys. · 1999 · 86 · 87110.1063/1.370817 ↗
7. J. Electrochem. Soc. · 1999 · 146 · 26610.1149/1.1391597 ↗
8. Appl. Phys. Lett. · 2002 · 80 · 273410.1063/1.1468916 ↗
9. IEEE Electron Device Lett. · 2002 · 23 · 18510.1109/55.992833 ↗
10. IEEE Microw. Wirel. Compon. Lett. · 2003 · 13 · 43110.1109/LMWC.2003.818532 ↗
11. Appl. Phys. Lett. · 2003 · 82 · 287410.1063/1.1569985 ↗
12. IEEE Electron Device Lett. · 2002 · 23 · 51410.1109/LED.2002.1004230 ↗
13. J. Appl. Phys. · 2003 · 94 · 55110.1063/1.1579550 ↗
14. IEEE Electron Device Lett. · 2005 · 26 · 72810.1109/LED.2005.856708 ↗
15. J. Vac. Sci. Technol. A · 2004 · 22 · 65510.1116/1.1722633 ↗
16. J. Electrochem. Soc. · 2004 · 151 · F16210.1149/1.1752935 ↗
17. Mater. Sci. Semicond. Process. · 2004 · 7 · 22710.1016/j.mssp.2004.09.018 ↗
18. Microelectron. Eng. · 2005 · 80 · 31310.1016/j.mee.2005.04.018 ↗
19. IEEE Electron Device Lett. · 2003 · 24 · 6310.1109/LED.2002.808159 ↗
20. J. Appl. Phys. · 2004 · 96 · 171910.1063/1.1766412 ↗
21. J. P. Sénateur, R. Madar, F. Weiss, O. Thomas, and A. Abrutis, French Patent No. FR 2707671 (1993),
22. European Patent No. EP 730671 (1994),
23. U.S. Patent No. US 945162 (1999).
24. Guilloux-Viry · 2002 · 169
25. Thin Solid Films · 1998 · 318 · 25210.1016/S0040-6090(97)01171-1 ↗
26. Nucl. Instrum. Methods Phys. Res. B · 1997 · 121 · 34910.1016/S0168-583X(96)00538-1 ↗
27. Surf. Interface Anal. · 2002 · 34 · 47210.1002/sia.1341 ↗
28. Tech. Dig. - Int. Electron Devices Meet. · 1998 · 823
29. IEEE Electron Device Lett. · 2003 · 24 · 73010.1109/LED.2003.820664 ↗
30. J. Non-Cryst. Solids · 2002 · 303 · 10810.1016/S0022-3093(02)00975-4 ↗
31. IEEE Trans. Electron Devices · 2004 · 51 · 88610.1109/TED.2004.827367 ↗
32. J. Electrochem. Soc. · 2005 · 152 · F21710.1149/1.2109487 ↗
33. IEEE Electron Device Lett. · 2003 · 24 · 44210.1109/LED.2003.814024 ↗
34. IEEE Electron Device Lett. · 2003 · 24 · 6010.1109/LED.2002.807703 ↗
35. 2003 · 79
36. Microelectron. Reliab. · 2003 · 43 · 125910.1016/S0026-2714(03)00181-1 ↗
37. IEEE Electron Device Lett. · 2004 · 25 · 53810.1109/LED.2004.832785 ↗
38. Appl. Phys. Lett. · 2002 · 81 · 421810.1063/1.1522826 ↗
39. IEEE Electron Device Lett. · 2002 · 23 · 19110.1109/55.992835 ↗