journal article·2012-01

Effects of Ar plasma treatment for deposition of ruthenium film by remote plasma atomic layer deposition

Taeyong Park, Jaesang Lee, Jingyu Park, Heeyoung Jeon, Hyeongtag Jeon, Ki-Hoon Lee, Byung-Chul Cho, Moo-Sung Kim, Heui-Bok Ahn

Publisher page

Abstract

Ruthenium thin films were deposited on argon plasma-treated SiO2 and untreated SiO2 substrates by remote plasma atomic layer deposition using bis(ethylcyclopentadienyl)ruthenium [Ru(EtCp)2] as a Ru precursor and ammonia plasma as a reactant. The results of in situ Auger electron spectroscopy (AES) analysis indicate that the initial transient region of Ru deposition was decreased by Ar plasma treatment at 400 °C, but did not change significantly at 300 °C. The deposition rate exhibited linearity after continuous film formation and the deposition rates were about 1.7 Å/cycle and 0.4 Å/cycle at 400 °C and 300 °C, respectively. Changes of surface energy and polar and dispersive components were measured by the sessile drop test. The quantity of surface amine groups was measured from the surface nitrogen concentration with AES. Furthermore, the Ar plasma-treated SiO2 contained more amine groups and less hydroxyl groups on the surface than on untreated SiO2. Auger spectra exhibited chemical shifts by Ru-O bonding, and larger shifts were observed on untreated substrates due to the strong adhesion of Ru films.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. 10.1016/S0921-5107(01)00727-910.1016/S0921-5107(01)00727-9 ↗
2. 10.1116/1.130381210.1116/1.1303812 ↗
3. 10.1149/1.183819810.1149/1.1838198 ↗
4. 10.1063/1.12311910.1063/1.123119 ↗
5. 10.1016/j.mssp.2004.09.01110.1016/j.mssp.2004.09.011 ↗
6. 10.1149/1.211364710.1149/1.2113647 ↗
7. 10.1143/JJAP.39.634810.1143/JJAP.39.6348 ↗
8. 10.1149/1.164063310.1149/1.1640633 ↗
9. 10.1063/1.276776910.1063/1.2767769 ↗
10. 10.1149/1.220001110.1149/1.2200011 ↗
11. 10.1149/1.213844410.1149/1.2138444 ↗
12. 10.1149/1.164861210.1149/1.1648612 ↗
13. 10.1016/j.mee.2007.01.23910.1016/j.mee.2007.01.239 ↗
14. 10.1016/0040-6090(92)90874-B10.1016/0040-6090(92)90874-B ↗
15. 10.1038/nmat100010.1038/nmat1000 ↗
16. 10.1002/cvde.v9:110.1002/cvde.v9:1 ↗
17. 10.1016/S0040-6090(01)00762-310.1016/S0040-6090(01)00762-3 ↗
18. 10.1116/1.146900910.1116/1.1469009 ↗
19. 10.1016/j.tsf.2006.05.04910.1016/j.tsf.2006.05.049 ↗
20. 10.1063/1.293805210.1063/1.2938052 ↗
21. 10.1021/cr900056b10.1021/cr900056b ↗
22. 10.1116/1.56904210.1116/1.569042 ↗
23. M. Ohring,Materials Science of Thin Films, 2nd ed. (Academic, New York, 2002), pp. 386–399.
24. 10.1116/1.58008210.1116/1.580082 ↗
25. E. F. Vansant, P. Van Der Voort, K. C. Vrancken,Characterization and Chemical Modification of the Silica Surface(Elsevier, Amsterdam, 1995) pp. 59–131383–390.10.1016/S0167-2991(06)81508-9 ↗
26. 10.1021/la061898u10.1021/la061898u ↗