Extrinsic time-dependent dielectric breakdown of low-k organosilicate thin films from vacuum-ultraviolet irradiation
Source abstract
Abstract
In this work, the effect of vacuum ultraviolet (VUV) photon irradiation on the time-dependent dielectric breakdown (TDDB) of low-k organosilicate thin films was investigated, with particular emphasis on extrinsic TDDB (includes Cu migration effects). State-of-the-art low-k a-SiOC:H thin films were utilized because of their relevance as both an interlayer dielectric and as a candidate Cu capping-layer material. Synchrotron radiation was used to mimic VUV photon irradiation from processing plasmas without the presence of charged particles. TDDB characteristic lifetimes of the low-k a-SiOC:H dielectrics, before and after VUV photon exposure, were measured based on a Ti/a-SiOC:H/Cu metal-insulator-metal structure. The deterioration of extrinsic TDDB was observed in the film after exposure to VUV photons with 9 eV energy. The most notable degradation of the dielectric characteristic lifetime was found when the Cu electrode was used as an anode in the sample after 9.0 eV VUV photon exposure (photon fluence is 4.0 × 1015 photons/cm2). This is believed to be related to the Cu+ ions created by a VUV photon-assisted reaction. In the presence of an electric field, these Cu ions drift into the low-k dielectric and deteriorate TDDB performance.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Copper Interconnects and Reliability · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
University of Wisconsin-Madison Plasma Processing and Technology Laboratory and Department of Electrical and Computer Engineering, , Madison, Wisconsin 53706
Intel Corporation Logic Technology Development, , Hillsboro, Oregon 97124
National Synchrotron Radiation Research Center , Hsinchu 30076, Taiwan
Stanford University Department of Electrical Engineering, , Stanford, California 94305
Funding
National Science Foundationation
References (29)
Show source-provided references
1. Proc. Mater. Res. Soc. Symp. · 1999 · 565 · 10710.1557/PROC-565-107 ↗
2. Thin Solid Films · 2004 · 469–470 · 38810.1016/j.tsf.2004.08.161 ↗
3. J. Solid State Sci. · 2012 · 1 · N11510.1149/2.021206jss ↗
4. ECS Trans. · 2013 · 45 · 2710.1149/04531.0027ecst ↗
5. J. Appl. Phys. · 2013 · 113 · 04110110.1063/1.4765297 ↗
6. J. Solid State Sci. · 2015 · 4 · N306510.1149/2.0091501jss ↗
7. Appl. Phys. Lett. · 2011 · 99 · 20290310.1063/1.3660248 ↗
8. Appl. Phys. Lett. · 2015 · 106 · 01290410.1063/1.4905462 ↗
9. 2013
10. Appl. Phys. Lett. · 2010 · 97 · 25290110.1063/1.3529492 ↗
11. Appl. Phys. Lett. · 2015 · 107 · 23290510.1063/1.4937582 ↗
12. J. Solid State Sci. · 2015 · 4 · N302910.1149/2.0051501jss ↗
13. J. Non-Cryst. Solids · 2013 · 379 · 6710.1016/j.jnoncrysol.2013.07.028 ↗
14. Microelectron. Eng. · 2012 · 92 · 8310.1016/j.mee.2011.04.014 ↗
15. J. Vac. Sci. Technol., A · 2013 · 31 · 05082510.1116/1.4819316 ↗
16. M. T. Nichols, “The effects of processing induced damage on electrical conduction mechanisms and time-dependent dielectric breakdown of low-k organosilicates,” Doctor of Philosophy thesis (University of Wisconsin-Madison, 2013).
17. J. Appl. Phys. · 2014 · 116 · 04410310.1063/1.4891501 ↗
18. D. Pei, “The effects of vacuum ultraviolet irradiation on the electrical properties of porous low-k organosilicate glass,” Doctor of Philosophy thesis (University of Wisconsin-Madison, 2016).
19. Jpn. J. Appl. Phys., Part 1 · 2006 · 45 · 157010.1143/JJAP.45.1570 ↗
20. J. Vac. Sci. Technol., A · 2001 · 19 · 4510.1116/1.1335685 ↗
21. J. Electrochem. Soc. · 1986 · 133 · 124210.1149/1.2108827 ↗
22. Appl. Phys. Lett. · 2015 · 106 · 07290210.1063/1.4913485 ↗
23. Appl. Phys. Lett. · 2012 · 100 · 11290510.1063/1.3693526 ↗
24. Appl. Phys. Lett. · 2015 · 107 · 08290310.1063/1.4929702 ↗
25. J. Am. Chem. Soc. · 2005 · 127 · 950610.1021/ja050006u ↗
26. Phys. Rev. B · 1988 · 38 · 1132210.1103/PhysRevB.38.11322 ↗
27. J. Appl. Phys. · 2013 · 114 · 08410310.1063/1.4817917 ↗
28. 2006 · 484
29. Materials · 2012 · 5 · 160210.3390/ma5091602 ↗