journal article·2017-11-01

Self-catalyst assisted and catalyst-free epitaxial growth of InAs on Ge (111): Role of substrate surface and evolution of polytypism

Suparna Pal, Chandrachur Mukherjee, Vasant G. Sathe, Ravi Kumar, Pragya Tiwari, Vijay Kumar Dixit, Tarun Kumar Sharma

Publisher page

Abstract

In the present work, the authors report on the role of a self-catalyst (indium) and a substrate surface in various growth mechanisms and the crystalline structure of InAs nucleating layers on Ge (111) using metal organic vapor phase epitaxy. This study opens up the possibility of direct integration of InAs with Ge (111) substrates for next generation optoelectronic and microelectronic device applications. Different nucleation modes like droplet-epitaxy (DE), Volmer–Weber (VW), and Frank–Van der Merwe (FM) modes are observed in various growth windows. DE and FM modes are the dominating nucleation modes at lower growth temperature (400–470 °C) with the assistance of indium catalysts, while the VW mode dominates at higher growth temperature (470–540 °C). Three dimensional faceted structures are formed with varying densities in the overall growth temperature range of 400–540 °C, which is attributed to various factors like surface strain of the indium adatom covered Ge (111) surface, indium surface diffusion, and twin defect formation. High resolution x-ray diffraction identifies the twin formation at low growth temperature. Raman mapping reveals that InAs nano-/microstructures grow with a zinc blende-wurtzite polytypic crystal structure at higher growth temperature and arsenic-rich conditions. A comparison is made on the growth modes, morphology, and polytypism in InAs nanostructures, which are grown on Ge (111) and Si (111) substrates under identical conditions. Low surface diffusivity of indium on the Ge substrate and InAs/Ge interface energy are proposed as the main factors for the inhibition of anisotropic axial growth of InAs on Ge via the vapor-liquid-solid mode, while they succeed on the Si substrate.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Nanowire Synthesis and Applications · Semiconductor Quantum Structures and Devices · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Optical Coatings Laboratory, Advanced Lasers and Optics Division, Raja Ramanna Centre for Advanced Technology , Indore 452013, M.P., India and , Anushakti Nagar, Mumbai 400094, India

Homi Bhabha National Institute, Training School Complex , Indore 452013, M.P., India and , Anushakti Nagar, Mumbai 400094, India

UGC-DAE Consortium for Scientific Research , Khandwa Road, Indore 452001, M.P., India

Semiconductor Materials Laboratory, Materials Science Section, Raja Ramanna Centre for Advanced Technology , Indore 452013, M.P., India and , Anushakti Nagar, Mumbai 400094, India

Lithography and Microscopy Laboratory, Synchrotron Utilization Section, Raja Ramanna Centre for Advanced Technology , Indore 452013, M.P., India and , Anushakti Nagar, Mumbai 400094, India

References (44)

Show source-provided references
1. J. Cryst. Growth · 2008 · 310 · 342810.1016/j.jcrysgro.2008.05.003 ↗
2. Semicond. Sci. Technol. · 2013 · 28 · 01502510.1088/0268-1242/28/1/015025 ↗
3. Nat. Photonics · 2011 · 5 · 41610.1038/nphoton.2011.120 ↗
4. Nano Lett. · 2009 · 9 · 292610.1021/nl901270n ↗
5. Nano Lett. · 2009 · 9 · 368910.1021/nl901348d ↗
6. Nanoscale Res. Lett. · 2010 · 5 · 3110.1007/s11671-009-9439-y ↗
7. J. Electron. Mater. · 2000 · 29 · 8010.1007/s11664-000-0099-z ↗
8. J. Cryst. Growth · 1998 · 195 · 65510.1016/S0022-0248(98)00652-6 ↗
9. Phys. Status Solidi C · 2012 · 9 · 32210.1002/pssc.201100252 ↗
10. IEEE Trans. Electron Devices · 1999 · 46 · 211610.1109/16.792006 ↗
11. J. Phys.: Conf. Ser. · 2008 · 100 · 04201710.1088/1742-6596/100/4/042017 ↗
12. Appl. Phys. Lett. · 2012 · 100 · 05211310.1063/1.3682314 ↗
13. Appl. Phys. Lett. · 2008 · 92 · 06311210.1063/1.2837191 ↗
14. Phys. Rev. B · 2007 · 76 · 15340110.1103/PhysRevB.76.153401 ↗
15. Appl. Phys. Lett. · 2006 · 89 · 06311910.1063/1.2336599 ↗
16. J. Appl. Phys. · 1993 · 73 · 740710.1063/1.354033 ↗
17. Nat. Mater. · 2004 · 3 · 76910.1038/nmat1235 ↗
18. Nano Lett. · 2015 · 15 · 725310.1021/acs.nanolett.5b02165 ↗
19. ECS Trans. · 2016 · 75 · 26510.1149/07505.0265ecst ↗
20. J. Alloy Compd. · 2015 · 646 · 39310.1016/j.jallcom.2015.05.265 ↗
21. Appl. Surf. Sci. · 2016 · 372 · 7010.1016/j.apsusc.2016.03.017 ↗
22. Nano Lett. · 2010 · 10 · 90810.1021/nl903688v ↗
23. Nano Lett. · 2010 · 10 · 349410.1021/nl101632a ↗
24. Phys. Rev. B · 2009 · 80 · 24532410.1103/PhysRevB.80.245324 ↗
25. Appl. Phys. Lett. · 2004 · 85 · 589310.1063/1.1839642 ↗
26. Appl. Phys. Lett. · 2007 · 90 · 20310510.1063/1.2737123 ↗
27. Appl. Phys. Lett. · 1996 · 69 · 77610.1063/1.117888 ↗
28. Phys. Rev. B · 1989 · 40 · 390510.1103/PhysRevB.40.3905 ↗
29. Appl. Phys. A · 1997 · 65 · 52510.1007/s003390050619 ↗
30. J. Vac. Sci. Technol., B · 1993 · 11 · 77910.1116/1.586787 ↗
31. Appl. Phys. Lett. · 2012 · 100 · 19210610.1063/1.4711783 ↗
32. J. Cryst. Growth · 1995 · 154 · 16310.1016/0022-0248(95)00884-5 ↗
33. Mater. Sci. Eng. B · 1999 · 67 · 2310.1016/S0921-5107(99)00205-6 ↗
34. Philos. Trans. R. Soc. London · 1805 · 95 · 6510.1098/rstl.1805.0005 ↗
35. J. Nano-Electron. Phys. · 2014 · 6 · 02010
36. J. Phys. D: Appl. Phys. · 2013 · 46 · 03530610.1088/0022-3727/46/3/035306 ↗
37. J. Vac. Sci. Technol., B · 2000 · 18 · 156610.1116/1.591427 ↗
38. Appl. Phys. Lett. · 2014 · 104 · 09210110.1063/1.4867526 ↗
39. Nano Lett. · 2011 · 11 · 148310.1021/nl1041512 ↗
40. Phys. Status Solidi RRL · 2011 · 5 · 15610.1002/pssr.201105055 ↗
41. Phys. Rev. B · 2011 · 84 · 15530110.1103/PhysRevB.84.155301 ↗
42. Phys. Rev. B · 2011 · 84 · 08531810.1103/PhysRevB.84.085318 ↗
43. Fisher · 199810.4028/b-04kxlP ↗
44. J. Appl. Phys. · 2009 · 106 · 06353410.1063/1.3226860 ↗