The authors report the simultaneous formation and transfer of GaAsN nanostructure layers to alternative substrates, a process termed “ion-cut synthesis.” Ion-cut synthesis is induced by nitrogen ion implantation into GaAs (GaAs:N), followed by spin-on-glass (SOG) mediated wafer bonding and high temperature rapid thermal annealing (RTA). Due to the low ion-matrix diffusivity of GaAs:N, RTA induces the formation of both nanostructures and gas bubbles. The gas bubble pressure induces the formation and propagation of cracks, resulting in transfer of the nanostructured layer. The authors discuss the critical role of the physical properties and the thicknesses of the substrates and the SOG layer to the achievement of ion-cut synthesis.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Semiconductor materials and devices · Nanowire Synthesis and Applications · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Michigan Department of Mechanical Engineering, University of Michigan, Ann Arbor, Michigan 48109-2125, USA and Department of Materials Science and Engineering, , Ann Arbor, Michigan 48109-2136, USA

University of Michigan Department of Materials Science and Engineering, University of Michigan, Ann Arbor, Michigan 48109-2136, USA and Department of Physics, , Ann Arbor, Michigan 48109-1040, USA

University of Michigan Department of Materials Science and Engineering, , Ann Arbor, Michigan 48109-2136, USA

National Institute of Standards and Technology Polymers Division, , Gaithersburg, Maryland 20899, USA

Los Alamos National Laboratory Materials Science and Technology Division, , Los Alamos, New Mexico 87545, USA

References (32)

Show source-provided references
1. Electron. Lett. · 1995 · 31 · 120110.1049/el:19950805 ↗
2. Appl. Phys. Lett. · 1997 · 71 · 276710.1063/1.120127 ↗
3. Appl. Phys. Lett. · 2006 · 89 · 15192210.1063/1.2361182 ↗
4. Appl. Phys. Lett. · 1998 · 72 · 108610.1063/1.120945 ↗
5. J. Appl. Phys. · 2005 · 97 · 08352710.1063/1.1865318 ↗
6. Appl. Phys. Express · 2009 · 2 · 02220110.1143/APEX.2.022201 ↗
7. Appl. Phys. Lett. · 2001 · 78 · 126710.1063/1.1342212 ↗
8. J. Electron. Mater. · 2003 · 32 · 82910.1007/s11664-003-0196-x ↗
9. Mater. Sci. Eng., B · 1997 · 46 · 34910.1016/S0921-5107(96)02004-1 ↗
10. Electron. Lett. · 1998 · 34 · 40710.1049/el:19980295 ↗
11. Electron. Lett. · 1999 · 35 · 67510.1049/el:19990477 ↗
12. J. Electron. Mater. · 2000 · 29 · 91610.1007/s11664-000-0181-6 ↗
13. Thin Solid Films · 2002 · 403–404 · 55810.1016/S0040-6090(01)01570-X ↗
14. Appl. Phys. Lett. · 2000 · 76 · 126110.1063/1.126003 ↗
15. Electron. Lett. · 1999 · 35 · 47710.1049/el:19990354 ↗
16. J. Electron. Mater. · 2001 · 30 · 83410.1007/s11664-001-0067-2 ↗
17. Microelectron. Eng. · 1997 · 36 · 23310.1016/S0167-9317(97)00055-5 ↗
18. Nucl. Instrum. Methods Phys. Res. B · 1996 · 108 · 31310.1016/0168-583X(95)01056-4 ↗
19. Thin Solid Films · 2002 · 403–404 · 50010.1016/S0040-6090(01)01664-9 ↗
20. Semiconductors · 2000 · 34 · 96510.1134/1.1188109 ↗
21. J. Appl. Phys. · 2002 · 92 · 401210.1063/1.1504177 ↗
22. Appl. Phys. Lett. · 2004 · 85 · 277410.1063/1.1803940 ↗
23. J. Vac. Sci. Technol. B · 2004 · 22 · 98910.1116/1.1715030 ↗
24. Appl. Phys. Lett. · 2011 · 99 · 09310810.1063/1.3617464 ↗
25. Appl. Phys. Lett. · 2009 · 95 · 11191210.1063/1.3224199 ↗
26. Adv. Mater. · 2007 · 19 · 70510.1002/adma.v19:5 ↗
27. MRS Bull. · 2007 · 32 · 40010.1557/mrs2007.63 ↗
28. Electron Lett. · 2000 · 36 · 67710.1049/el:20000507 ↗
29. Annu. Rev. Mater. Res. · 2010 · 40 · 46910.1146/annurev-matsci-070909-104448 ↗
30. Int. J. Fracture · 1990 · 43 · 110.1007/BF00018123 ↗
31. Electron. Lett. · 1998 · 34 · 40810.1049/el:19980265 ↗
32. 1985