journal article·1997-01-01

Dominant monohydride bonding in hydrogenated amorphous silicon thin films formed by plasma enhanced chemical vapor deposition at room temperature

Easwar Srinivasan, Daniel A. Lloyd, Gregory N. Parsons

Publisher page

Abstract

Hydrogenated amorphous silicon (a-Si:H) prepared by plasma enhanced chemical vapor deposition (PECVD) with silane, typically shows significant dihydride bonding and high defect density when the substrate temperature is less than 200 °C. Monohydride bonding is associated with low defect densities, and is usually observed only above 250 °C. Using rf (13.56 MHz) PECVD, we have deposited a-Si:H films at a substrate temperature of 35 °C using silane diluted with helium, and found that films with dominant monohydride bonding can be deposited without significant substrate heating. A specific ion enhanced reaction mechanism that is consistent with the results is proposed. As deposited, the films with predominant monohydride bonding show low dark conductivity (10−9 S/cm) and low photoconductivity (10−7 S/cm under 100 mW/cm2 while light illumination). Annealing the films for 3–4 h at 150 °C, resulted in an improved photoconductivity with photo to dark conductivity ratio near 105. These films may be valuable for the fabrication of thin film electronics on novel substrates compatible with only low temperature processes.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Thin-Film Transistor Technologies · Metallic Glasses and Amorphous Alloys · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemical Engineering, North Carolina State University, Raleigh, North Carolina 27695

References

Reference metadata was not supplied for this record.