Electron escape depth variation in thin SiO2 films measured with variable photon energy
Source abstract
Abstract
We have used a double crystal monochromator at the Stanford Synchrotron Radiation Laboratory to study the Si/SiO2 interface using photon energies of hν=1950–3700 eV. This photon energy range allows interfaces to be observed through oxide layers 50 Å thick or more. Variations in electron escape depth and/or oxide density as a function of distance from the interface are observed over the entire kinetic energy range (100–3600 eV). We attribute these differences to a strained oxide layer near the interface.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electron and X-Ray Spectroscopy Techniques · Advancements in Photolithography Techniques · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Jet Propulsion Laboratory, California Institute of Technology, Pasadena, California 91109
Stanford Synchrotron Radiation Laboratory, Stanford, California 94305
References
Reference metadata was not supplied for this record.