Photochemical oxidation of (Hg, Cd)Te: Passivation processes and characteristics
Source abstract
Abstract
We have demonstrated the controlled growth of photochemical native oxide on (Hg, Cd)Te by the UV photodissociation of N2O. The initial growth rate is ∼7Å/min, is insensitive to temperature over the range from 40 to 100 °C, and is dependent on the surface Hg concentration. Encapsulation of the native oxide with photochemical SiO2 results in a degradation of the (Hg, Cd)Te–native oxide interface electrical properties. The presence of photochemical HgO between the native oxide and SiO2 results in superior (Hg, Cd)Te surface electronic properties. However, MOS structures comprising SiO2 on a double layer of HgO on photochemical native oxide undergo an electrical degradation at room temperature, likely owing to reactions between HgO and the native oxide or (Hg, Cd)Te substrate.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Advanced Semiconductor Detectors and Materials · Gas Sensing Nanomaterials and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chemistry and Physics Laboratory, The Aerospace Corporation, Los Angeles, California 90009