journal article·1992-07-01

Atomic force microscope imaging for process characterization in diamond film deposition

Donald A. Chernoff, Henry Windischmann

Publisher page

Abstract

Atomic force microscope (AFM) images are presented for diamond films deposited using two processes. Films were deposited on polished Si from a CH4–H2 mixture by microwave plasma chemical vapor deposition (CVD) for CH4 concentrations in the range 0.4%–2.0%. At the lowest CH4 concentration, the film surface was rough (Rq = 80 nm) and contained many grains wider than 1 μ and taller than 0.4 μ. At the highest CH4 concentration, the growth of large grains was suppressed, producing much smoother films (Rq = 25 nm), which may be suitable as mask substrates for x-ray lithography. Filament-assisted CVD was also used; deposition was halted before a continuous film formed. The tallest grains (100–200-nm high) were clustered in intersecting linear arrays corresponding to marks made by diamond-polishing (seeding). Features a few nm high found in flat regions may be diamond nuclei on bare Si formed much later.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Force Microscopy Techniques and Applications · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Advanced Surface Microscopy, Inc., Indianapolis, Indiana 46220-4955

BP America, Research Center, Cleveland Ohio 44128

References

Reference metadata was not supplied for this record.