Vacuum annealing studies of thin TiC layers on steels
Source abstract
Abstract
Single-phase δ-TiC and two-phase (α-Ti and δ-TiC) layers deposited by activated reactive evaporation and biased activated reactive evaporation methods have been exposed to 1-h vacuum annealing in the temperature range 700–1400 K. The effects of that annealing on the chemical composition, morphology, microstructure, lattice parameter of the δ-TiC phase, and mechanical characteristics (microhardness and adhesion) have been investigated. Three ranges of the annealing temperatures have been ascertained in which particular changes of the above characteristics are occurring, viz., 700–900, 900–1100, and 1100–1400 K. Apart from these results, which could have been expected on the basis of the recovery, recrystallization, and grain-coarsening processes, the crucial effects of the diffusion of C atoms from the steel substrate to the deposit have also been ascertained.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Materials Science and Technology of Metals, Technical University of Lodz, Zwirki 36, 90–924 Lodz, Poland
Institute of Heat Engineering, Da̢browskiego 113, 93–208 Lodz, Poland
References
Reference metadata was not supplied for this record.