Dopant diffusion in silicides: Effect of diffusion paths
Source abstract
Abstract
While dopants implanted in well annealed WSi2 show no lattice diffusion and only limited grain-boundary diffusion at temperatures up to 900 °C, on the contrary, rapid diffusion is observed at temperatures as low as 300 °C when the implantation takes place in the as-deposited amorphous silicide. Diffusion appears to be always accompanied by crystallization, although the inverse is not true: in particular, the diffusion of Sb occurs only at temperatures in excess of what is necessary to cause crystallization. The diffusion coefficients vary in reverse proportion to the size of the diffusing atoms, so that approximately equal coefficients for B, P, As, and Sb require respective temperatures of 350, 400, 450, and 500 °C. The diffusion coefficient of As at 500 °C is estimated at 1 × 10−14 cm2 s−1. The apparent activation energy for grain-boundary diffusion is close to 2.4 eV for P, As, and Sb.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and interfaces · Silicon and Solar Cell Technologies · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
IBM Research Center, Yorktown Heights, New York 10598
ENSPG, BP 46, 38402 Saint Martin d’Hères, France
Laboratoire de Métallurgie, URA 443/CNRS, Université Saint Jérôme, 13397 Marseille, France
References
Reference metadata was not supplied for this record.