Oxidation-enhanced roughening of thin Co films during sputtering by O+2 ions
Source abstract
Abstract
Substantial variations in the erosion rate during low energy (5.5–10.5 keV) O+2 sputtering of polycrystalline Co thin films are demonstrated by crater depth measurements as a function of sputtering time. At normal incidence the erosion rate is constant, while for oblique angles (≤55°, with respect to surface normal) the rate is between ∼30% and 75% higher at the surface compared to that in the ‘‘bulk.’’ A clear relationship between the width of the preequilibrium region and the sputtering-induced roughness is shown, as revealed by surface stylus profilometry and atomic force microscopy measurements. Sputtering by Ar+ ions, where no chemical compounds form, results in significantly smoother craters and the erosion rate is constant. The development of the preequilibrium region during O+2 sputtering of Co is attributed to oxidation-induced roughening of Co. A model is proposed for the oxidation-enhanced roughening, which is further supported by results obtained from Rutherford backscattering spectrometry measurements of oxygen incorporation during O+2 bombardment and Ar+ sputtering combined with oxygen flooding.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ion-surface interactions and analysis · Fusion materials and technologies · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Solid State Electronics, Royal Institute of Technology, P. O. Box E229, S-164 40 Kista-Stockholm, Sweden
Department of Electronic Materials Engineering, Research School of Physical Sciences and Engineering, Australian National University, Canberra, ACT 0200, Australia
Solid State Electronics, Royal Institute of Technology, P.O. Box E229, S-164 40 Kista-Stockholm, Sweden
References
Reference metadata was not supplied for this record.