Crystallization and stress relaxation behaviors of UHMWPE/CNT fibers
Source abstract
Abstract
Crystallization and stress relaxation behaviors of ultrahigh molecular weight polyethylene (UHMWPE) doped with carbon nanotubes (CNTs) have been investigated by X‐ray diffraction, differential scanning calorimetry (DSC) and single strand strength testing. Compared with UHMWPE, crystallinity of the UHMWPE/CNT composites significantly increases from 71.95 to 82.92% while crystallization activation energy decreases from 679.4 to 535.8 KJ/mol. CNTs as the nucleating agent changes the nucleation type of UHMWPE from homogenous to heterogeneous and accelerates the nucleation and growing of crystalline grains. Above crystallization changes also affect the mechanical properties of the UHMWPE/CNTs composites. Stress relaxation testing indicates that the relaxation stability of UHMWPE/CNT composites increases while the relaxation rate decreases. J. VINYL ADDIT. TECHNOL., 24:229–232, 2018. © 2016 Society of Plastics Engineers
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Carbon Nanotubes in Composites · Polymer crystallization and properties · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Engineering Research Center for Eco‐Dyeing & Finishing of Textiles, Ministry of Education, Zhejiang Sci‐Tech University Hangzhou 310018 People's Republic of China
Rongsheng Petrochemical Co., Ltd Hangzhou 311247 People's Republic of China
Funding
Natural Science Foundation of Zhejiang Province
References (16)
Show source-provided references
1. 10.1002/1097-4636(2000)53:4<414::AID-JBM16>3.0.CO;2-M10.1002/1097-4636(2000)53:4<414::AID-JBM16>3.0.CO;2-M ↗
2. Goodridge R.D. · J. Mater. Proc. Technol. · 2012 · 210 · 5785
3. 10.1007/s12221-014-0480-910.1007/s12221-014-0480-9 ↗
4. 10.1002/adma.20040197710.1002/adma.200401977 ↗
5. 10.1007/s12034-007-0061-210.1007/s12034-007-0061-2 ↗
6. 10.1166/jnn.2008.09210.1166/jnn.2008.092 ↗
7. 10.1007/s11249-007-9219-810.1007/s11249-007-9219-8 ↗
8. 10.1007/s12221-013-1635-910.1007/s12221-013-1635-9 ↗
9. 10.1023/B:TRIL.0000015206.21688.8710.1023/B:TRIL.0000015206.21688.87 ↗
10. 10.1007/s11249-010-9610-810.1007/s11249-010-9610-8 ↗
11. 10.1016/j.polymer.2006.01.02010.1016/j.polymer.2006.01.020 ↗
12. 10.1002/sia.214810.1002/sia.2148 ↗
13. Wang X.‐P. · Synth. Technol. Appl. · 2005 · 20 · 16
14. 10.6028/jres.057.02610.6028/jres.057.026 ↗
15. 10.1134/1.168786310.1134/1.1687863 ↗
16. 10.1016/j.jnoncrysol.2004.07.00510.1016/j.jnoncrysol.2004.07.005 ↗