journal article·2022-05Open access

Thermal stability of filler‐based ethylene/vinyl acetate/vinyl alcohol terpolymer in nitroplasticizer oxidative environment

Dali Yang, Kevin C. Henderson, Robin M. Pacheco, Kevin M. Hubbard, David J. Devlin

Abstract

Abstract To study the thermal stability of ethylene/vinyl acetate/vinyl alcohol (EVA‐OH) composite with filler particles, systematic thermogravimetric analysis (TGA) investigation was conducted in both nonisothermal and isothermal modes. The effect of polymer concentration on the aging behavior of EVA‐OH was investigated in the nitroplasticizer (NP) environment. Fourier transform infrared spectroscopy was used to probe chemical structural changes in the EVA‐OH polymer before and after thermal aging. The results suggest that filler addition accelerates the rate of NP exudation out of the EVA‐OH composites and deteriorates the thermal stability of NP at moderate temperatures (up to 70°C). The degradation of NP, in turn, accelerates the degradation of EVA‐OH polymer in its composite form through oxidation and hydrolysis indicating the importance of antioxidants in such phase blends.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Polymer Nanocomposites and Properties · Polymer crystallization and properties · Thermal and Kinetic Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

MST‐7: Engineered Materials, Division of Materials Science Los Alamos National Laboratory Los Alamos New Mexico USA

MPA‐Q: MPA‐Quantum, Division of Materials Physics and Application Los Alamos National Laboratory Los Alamos New Mexico USA

Sigma‐1: Fabrication Manufacturing Science, Division of Materials Science Los Alamos National Laboratory Los Alamos New Mexico USA

Funding

U.S. Department of Energy · National Nuclear Security Administration · Los Alamos National Laboratory

References (34)

Show source-provided references
1. Allen N. S. · Polym. Degrad. Stab. · 2001 · 71 · 14
2. E. A.Eastwood Kansas City Plant Report: KCP‐613‐6929 2004 72.
3. 10.1016/j.polymdegradstab.2011.08.01710.1016/j.polymdegradstab.2011.08.017 ↗
4. S. E.Letant T. S.Wilson C. T.Alviso W. S.IV A. M.Heather M.Pearson J. L.Herberg S. C.Chinn R. S.Maxwell LLNL‐TR‐420245 2009 27.
5. 10.1016/j.polymertesting.2012.08.01210.1016/j.polymertesting.2012.08.012 ↗
6. A.Provatas Aeronautical and Maritime Research Laboratory DSTO‐TR‐0996 2000 51.
7. 10.1016/j.polymdegradstab.2009.08.01110.1016/j.polymdegradstab.2009.08.011 ↗
8. 10.1002/app.2620710.1002/app.26207 ↗
9. 10.1002/prep.20039000010.1002/prep.200390000 ↗
10. 10.1002/app.4072910.1002/app.40729 ↗
11. 10.1016/j.polymdegradstab.2016.06.00710.1016/j.polymdegradstab.2016.06.007 ↗
12. 10.1002/prep.20190019410.1002/prep.201900194 ↗
13. 10.1016/j.polymdegradstab.2016.05.01710.1016/j.polymdegradstab.2016.05.017 ↗
14. 10.1016/0040-6031(93)80013-Z10.1016/0040-6031(93)80013-Z ↗
15. 10.1002/prep.20070001210.1002/prep.200700012 ↗
16. 10.1016/S1540-7489(02)80350-910.1016/S1540-7489(02)80350-9 ↗
17. 10.1039/b707604e10.1039/b707604e ↗
18. 10.1016/j.polymdegradstab.2019.10902010.1016/j.polymdegradstab.2019.109020 ↗
19. Yang D. · J. Appl Polym Sci · 2014 · 132 · 17
20. Patel M. · Polym. Test. · 2013 · 32 · 8
21. 10.1002/prep.20080020310.1002/prep.200800203 ↗
22. 10.1016/0040-6031(94)85058-510.1016/0040-6031(94)85058-5 ↗
23. Edgar A. · J. Energ Mater · 2020 · 21
24. Berman R. · 1976
25. Leea G.‐W. · Composites: Part A · 2006 · 37 · 8
26. 10.1016/S0014-3057(02)00064-210.1016/S0014-3057(02)00064-2 ↗
27. Marin M. L. · J. Thermal Anal · 1996 · 47 · 12
28. 10.5254/rct.14.8593010.5254/rct.14.85930 ↗
29. 10.1080/71377043510.1080/713770435 ↗
30. 10.1002/prep.1995020020210.1002/prep.19950200202 ↗
31. 10.1366/000370292412426810.1366/0003702924124268 ↗
32. Perry R. H. · 1984 · 20
33. 10.5772/2343610.5772/23436 ↗
34. 10.1002/vnl.2185910.1002/vnl.21859 ↗