Surface free energy and dynamic wettability of wood simultaneously treated with acidic dye and flame retardant
Source abstract
Abstract
The use of multifunctional wood for decorative purpose has grown increasingly popular in recent years. In this study, fast-growing poplar wood was treated with dye (0.5%) and flame retardant (0, 10, 20, and 30%) simultaneously to enhance its visual characteristic and safety. The dynamic wettability and surface free energy of wood samples were studied using S-D wetting model and van Oss–Chaudhury–Good (vOCG) method, respectively. Dye uptake, drug load, color difference, and combustion performance were determined. The treated wood was also characterized by infrared spectroscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The results indicated that the proposed treatment yields favorable adhesive spreading and penetration ability at the wood surface. The surface free energy of treated wood was higher than that of untreated wood, and the dye uptake, drug load, color difference, and limited oxygen index all increased after the proposed combination treatment compared to dye-only treated wood. The results also indicated that the flame retardant reacted chemically with the wood as the dye and flame retardant molecules diffused into the cell cavity, wood vessel, and aperture.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Lignin and Wood Chemistry · Wood Treatment and Properties · Flame retardant materials and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Gindl M, Reiterer A, Sinn G, Stanzl-Tschegg SE (2004) Effects of surface on wettability, surface chemistry, and adhesion of wood. Holz Roh Werkst 62:273–28010.1007/s00107-004-0471-4 ↗
2. Bryne LE, Wålinder MEP (2010) Ageing of modified wood. Part 1: wetting properties of acetylated, furfurylated, and thermally modified wood. Holzforschung 64:295–304
3. Xiong GB (2005) Study on dyeing, enhancement and dimensional stability of fast-growing poplar. Dissertation, Nanjing Forestry University, Nanjing
4. Jia Z (2012) The study of nano-CaCO3/fast-growing poplar composite and preparing building templates. Dissertation, Northeast Forestry University, Harbin
5. Subyakto, Kajimoto T, Hata T, Ishihara S, Kawai Shuichi, Getto H (1998) Improving fire retardancy of fast growing wood by coating with fire retardant and surface densification. Fire Mater 22:207–21210.1002/(SICI)1099-1018(199809/10)22:5<207::AID-FAM654>3.0.CO;2-S ↗
6. Taghiyari HR (2012) Fire-retarding properties of nano-silver in solid woods. Wood Sci Technol 46:939–95210.1007/s00226-011-0455-6 ↗
7. Pries M, Mai C (2013) Fire resistance of wood treated with a cationic silica sol. Eur J Wood Prod 71:237–24410.1007/s00107-013-0674-7 ↗
8. Sang BP, Min L, Dong WS, Sang ML, Jong IK (2014) Fire performance of carbonized medium density fiberboard manufactured at different temperatures. J Wood Sci 60:74–7910.1007/s10086-013-1379-6 ↗
9. Pan J, Mu J, Wu ZX, Zhang XT (2014) Effect of nitrogen–phosphorus fire retardant blended with Mg(OH)2/Al(OH)3 and nano-SiO2 on fire-retardant behavior and hygroscopicity of poplar. Fire Mater 38:817–82610.1002/fam.2224 ↗
10. Baharoğlu M, Nemli G, Sarı B, Bardak S, Ayrılmış N (2012) The influence of moisture content of raw material on the physical and mechanical properties, surface roughness, wettability, and formaldehyde emission of particleboard composite. Compos Part B 43:2448–245110.1016/j.compositesb.2011.10.020 ↗
11. Gindl M, Reiterer A, Sinn G, Stanzl-Tschegg SE (2004) Effects of surface ageing on wettability, surface chemistry, and adhesion of wood. Holz Roh Werkst 62:273–28010.1007/s00107-004-0471-4 ↗
12. Rathke J, Sinn G (2013) Evaluating the wettability of MUF resins and pMDI on two different OSB raw materials. Eur J Wood Prod 71:335–34210.1007/s00107-013-0675-6 ↗
13. Wang S, Zhang Y, Xing C (2007) Effects of drying method on the surface wettability of wood strands. Holz Roh Werkst 65:437–44210.1007/s00107-007-0191-7 ↗
14. Jennings JD, Zink-Sharp A, Kamke FA, Frazier CE (2005) Properties of compression densified wood. Part I: bond performance. J Adhes Sci Technol 19:1249–126110.1163/156856105774429055 ↗
15. Fang Q, Cui HW, Du GB (2016) Surface wettability, surface free energy, and surface adhension of microwave plasma-treated Pinus yunnaensis wood. Wood Sci Technol 50:285–29610.1007/s00226-015-0793-x ↗
16. De Gennes, PG (1985) Wetting: statics and dynamics. Rev Mod Phys 57:827–86310.1103/RevModPhys.57.827 ↗
17. Qin ZY, Gao Q, Zhang SF, Li JZ (2014) Surface free energy and dynamic wettability of differently machined poplar woods. BioResources 9:3088–3103
18. Qin TF, Yan HP (2001) A study on effect of esterification and graft copolymerization process on surface free energy of wood. Scientia Silvae Sinicae 37:97–100
19. Qin ZY, Chen H, Gao Q, Zhang SF, Li JZ (2015) Wettability of sanded and aged fast-growing poplar wood surfaces: I. surface free energy. BioResources 10:1008–1023
20. Zhang DR (2005) Study on producing technology of dyeing and fire-retardant glue-lumber. Dissertation. Beijing Forestry University, Beijing
21. Li WZ (2011) The preparation technology of flame retardant plywood with decorative and environmental concern. Dissertation. Beijing Forestry University, Beijing
22. Tang R, Yu Z, Luna M, Zhang Y, Qi C (2015) Mechanisms and properties of chitosan-assisted bamboo dyeing. BioResources 10:3326–3336
23. Zhang X, Mu J, Chu D, Zhao Y (2016) Synthesis of fire retardants based on N and P and poly (sodium silicate-aluminum dihydrogen phosphate) (PSADP) and testing the flame retardant properties of PSADP impregnated poplar wood. Holzforschung 70:341–35010.1515/hf-2014-0362 ↗
24. Romagnoli M, Segoloni E, Luna M, Margaritelli A, Gatti M, Santamaria U, Vinciguerra V (2013) Wood color in Lapacho (Tabebuia serratifolia): chemical composition and industrial implications. Wood Sci Technol 47:701–71610.1007/s00226-013-0534-y ↗
25. EN ISO 4589-2 (1996) Plastics—determination of burning behaviour by oxygen index—part 2, ambient temperatures. International Organization for Standardization, Geneva
26. van Oss CJ, Good RJ, Chaudhury MK (1988) Additive and nonadditive surface tension components and the interpretation of contact angle. Langmuir 4:884–89110.1021/la00082a018 ↗
27. van Oss CJ, Giese RF, Good RJ (1990) Reevaluation of the surface tension components and parameters of polyacetylene from contact angle of liquids. Langmuir 6:1711–171310.1021/la00101a017 ↗
28. Liptakova E, Kudela J (1994) Analysis of the wood-wettinh process. Holzforschung 48:139–14410.1515/hfsg.1994.48.2.139 ↗
29. Tang L, Zhang R, Zhou X, Pan M, Chen M, Yang X, Zhou P, Chen Z (2012) Dynamic adhesive wettability of poplar veneer with cold oxygen plasma treatment. BioResources 7:3327–333910.15376/biores.7.4.5211-5221 ↗
30. Topala I, Dumitrascu N (2007) Dynamics of the wetting process on dielectric barrier discharge (DBD)-treated wood surfaces. J Adhes Sci Technol 21:1089–109610.1163/156856107782105936 ↗
31. Xu HN, Shen QY, Ouyang XK, Yang LY (2010) Wetting of soy protein adhesives modified by urea on wood surfaces. Eur J Wood Prod 70:11–16
32. Shi SQ, Gardner DJ (2001) Dynamic adhesive wettability of wood. J Wood Fiber Sci 33:58–68
33. Kang H, Wang Z, Zhang W, Li J, Zhang S (2016) Phys ico-chemical properties improvement of soy protein isolate films through caffeic acid incorporation and tri-functional aziridine hybridization. Food Hydrocolloids 61:923–93210.1016/j.foodhyd.2016.07.009 ↗
34. Chu D, Mu J, Zhang L, Li Y (2016) Promotion effect of NP fire retardant pre-treatment on heat-treated poplar wood. Part 2: hygroscopicity, leaching resistance, and thermal stability. Holzforschung. doi: 10.1515/hf-2016-021310.1515/hf-2016-0213 ↗
35. Wang PQ, Tai DS, Liao JY, Li MD (1987) Wood chemistry. China Forestry Publishing House, Beijing
36. Wang X, Zhang Y, Yu Z, Qi C (2016) Properties of fast-growing poplar wood simultaneously treated with dye and flame retardant. Eur J Wood Prod. doi: 10.1007/s00107-016-1142-y10.1007/s00107-016-1142-y ↗
37. Li WZ, Yu ZM, Chen LY, Jiang XD (2010) Study on the discoloration laws of poplar veneer treated by BL-flame retardant. J Anhui Agri Sci 38:12057–12059
38. Wang X, Yu Z, Zhang Y, Wang F (2016) Dyeing and flame retardant properties of poplar veneer. J Northwest For Univ 31:276–280
39. Wang YL (2006) Application study of BL-environmental concerned fire-retardant in particleboard. Dissertation. Beijing Forestry University, Beijing
40. Zhang L (2007) The application study of BL-environmental friendly fire retardant on textile. Dissertation. Beijing Forestry University, Beijing
41. Arora S, Kumar M, Kumar M (2012) Catalytic effect of bases in impregnation of guanidine nitrate on Poplar (Populus) wood:flammability and multiple heating rate kinetic study. J Therm Anal Calorim 107:1277–128610.1007/s10973-011-1779-z ↗
42. Kumar M, Kumar M, Arora S (2013) Thermal degradation and flammability studies of wood coated with fly ash intumescent composites. J Indian Acad Wood Sci 10:125–13310.1007/s13196-013-0105-8 ↗
43. Chen LY (2010) The preparation technology of flame-retarded plywood treated with BL flame retardant. Dissertation. Beijing Forestry University, Beijing
44. Jiang ZH, Yu WJ, Yu YL (2005) A study on wettability of bamboo wood surface. J Bamboo Res 24:31–38
45. Stehr M, Gardner DJ, Wålinder MEP (2001) Dynamic wettability of different machined wood surface. J Adhes 76:185–20010.1080/00218460108029625 ↗
46. Li H, Yu ZM (2005) Combinative mechanism between dyestuff and wood. J Beijing For Univ 27:78–81
47. Wang XQ, Yu ZM, Zhang Y (2016) Effect of pretreatment on dyeing and fire-retarding properties of poplar veneers. J Fujian Agric For Univ 45:1–5
48. Baldan A (2012) Adhesion phenomena in bonded joints. Int J Adhes Adhes 38:95–11610.1016/j.ijadhadh.2012.04.007 ↗
49. Wei SY, Shi JY, Gu JY, Wang D, Zhang YH (2016) Dynamic wettability of wood surface modified by acidic dyestuff and fixing agent. J Appl Surf Sci 258:1995–199910.1016/j.apsusc.2011.05.072 ↗