journal article·2019-12Open access

Effects of modification with a combination of styrene-acrylic copolymer dispersion and sodium silicate on the mechanical properties of wood

Thi Tham Nguyen, Zefang Xiao, Wenbo Che, Hien Mai Trinh, Yanjun Xie

Journal of Wood Science· Volume 65· Issue 1

Abstract

Poplar ( Populus adenopoda Maxim.) and radiata pine ( Pinus radiata Don.) woods were treated with an aqueous solution containing styrene-acrylic copolymer (SAC) dispersion and sodium silicate (SS). The modifying effects on the mechanical properties of wood were investigated with 10% SAC and varying concentrations of SS. The SAC and the SS deposition occurred in the cell lumina and condensed under catalysis at elevated temperature, as evidenced by scanning electron microscopy. The wood treated with SAC and SS exhibited a moisture content about 2 times higher than that of the untreated control under 95% relative humidity due to the introduction of hygroscopic silicate. The modulus of rupture (MOR) and modulus of elasticity (MOE) in the bending, compressive strength, surface hardness, tensile strength, and shear strength of the wood were improved up to 83.9, 82.3, 72.7, 48.3, 38.4, and 53.1%, respectively. However, the impact strength decreased by 39.4% due to the treatments. Accordingly, the combined treatment with SAC/SS has a potential application in the improvement of the wood quality, but the reduction in impact strength could limit its utilization in products for which high dynamic strength is required.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Wood Treatment and Properties · Lignin and Wood Chemistry · Tree Root and Stability Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Furuno T, Shimada K, Uehara T, Jodai S (1992) Combination of wood and silicate, 2: wood-mineral composites using water glass and reactants of barium chloride, boric acid, and borax, and their properties. J Jap Wood Res Soc 38(5):448–457
2. Böttcher H, Jagota C, Trepte J, Kallies KH, Haufe H (1999) Sol–gel composite films with controlled release of biocides. J Control Release 60(1):57–6510.1016/S0168-3659(99)00053-X ↗
3. Mai C, Militz H (2004) Modification of wood with silicon compounds. Treatment systems based on organic silicon compounds—a review. Wood Sci Technol 37(6):453–46110.1007/s00226-004-0225-9 ↗
4. Fan F, Xia Z, Li Q, Li Z, Chen H (2013) Thermal stability of phosphorus-containing styrene–acrylic copolymer and its fire retardant performance in waterborne intumescent coatings. J Therm Anal Calorim 114(3):937–94610.1007/s10973-013-3099-y ↗
5. Xiao Z, Xu J, Mai C, Militz H, Wang Q, Xie Y (2016) Combustion behavior of Scots pine (Pinus sylvestris L.) sapwood treated with a dispersion of aluminum oxychloride-modified silica. Holzforschung 70(12):1165–117310.1515/hf-2016-0062 ↗
6. Dong Y, Yan Y, Zhang S, Li J, Wang J (2015) Flammability and physical–mechanical properties assessment of wood treated with furfuryl alcohol and nano-SiO2. Eur J Wood Wood Prod 73(4):457–46410.1007/s00107-015-0896-y ↗
7. Furuno T, Uehara T, Jodai S (1993) Combinations of wood and silicate, 3: some properties of wood-mineral composites using the water glass-boron compound system. J Jap Wood Res Soc 39(5):561–570
8. Šimkovic I, Martvon̆ová H, Maníková D, Grexa O (2005) Flame retardance of insolubilized silica inside of wood material. J Appl Polym Sci 97(5):1948–195210.1002/app.21962 ↗
9. Slimak KM, Slimak RA (2007) Process of using sodium silicate to create fire retardant products. US Patent 7,297.411 B2. 20 Nov 2007
10. Pereyra AM, Giudice CA (2009) Flame-retardant impregnants for woods based on alkaline silicates. Fire Safety J 44(4):497–50310.1016/j.firesaf.2008.10.004 ↗
11. Hazarika A, Maji TK (2014) Properties of softwood polymer composites impregnated with nanoparticles and melamine formaldehyde furfuryl alcohol copolymer. Polym Eng Sci 54(5):1019–102910.1002/pen.23643 ↗
12. Yan Y, Dong Y, Li J, Zhang S, Xia C, Shi SQ, Cai L (2015) Enhancement of mechanical and thermal properties of Poplar through the treatment of glyoxal-urea/nano-SiO2. RSC Adv 5(67):54148–5415510.1039/C5RA07294H ↗
13. Shi J, Li J, Zhou W, Zhang D (2007) Improvement of wood properties by urea-formaldehyde resin and nano-SiO2. Front For China 2(1):104–10910.1007/s11461-007-0017-0 ↗
14. Jiang T, Feng X, Wang Q, Xiao Z, Wang F, Xie Y (2014) Fire performance of oak wood modified with N-methylol resin and methylolated guanylurea phosphate/boric acid-based fire retardant. Constr Build Mater 72:1–610.1016/j.conbuildmat.2014.09.004 ↗
15. Tilak G (1985) Thermosetting acrylic resins-a literature review. Prog Org Coat 13(5):333–34510.1016/0033-0655(85)80014-5 ↗
16. Chiantore O, Lazzari M (1996) Characterization of acrylic resins. Int J Polym Anal Ch 2(4):395–40810.1080/10236669608033358 ↗
17. Chuang CS, Tsai KC, Wang MK, Ko CH, Ing-Luen S (2009) Impact of the intumescent formulation of styrene acrylic-based coatings on the fire performance of thin painted red lauan (Parashorea spp.) plywood. Eur J Wood Wood Prod 67(4):407–41510.1007/s00107-009-0338-9 ↗
18. Zhong Z, Yu Q, Yao H, Wu W, Feng W, Yu L, Xu Z (2013) Study of the styrene–acrylic emulsion modified by hydroxyl-phosphate ester and its stoving varnish. Prog Org Coat 76(5):858–86210.1016/j.porgcoat.2013.02.008 ↗
19. Che W, Xiao Z, Han G, Zheng Z, Xie Y (2018) Radiata pine wood treatment with a dispersion of aqueous styrene/acrylic acid copolymer. Holzforschung 72(5):387–39710.1515/hf-2017-0142 ↗
20. Siau JF (1984) Basic wood–moisture relationships. Transport processes in wood. Springer, Berlin, pp 1–3410.1007/978-3-642-69213-0 ↗
21. Gezici-Koç Ö, Erich SJ, Huinink HP, van der Ven LG, Adan OC (2017) Bound and free water distribution in wood during water uptake and drying as measured by 1D magnetic resonance imaging. Cellulose 24(2):535–55310.1007/s10570-016-1173-x ↗
22. Alma M, Maldas D, Hafizo H (1995) Water repellency of several wood species impregnated with vinyl monomers. Int J Polym Mater 30(3–4):159–16510.1080/00914039508028594 ↗
23. Kartal SN, Hwang WJ, Yamamoto A, Tanaka M, Matsumura K, Imamura Y (2007) Wood modification with a commercial silicon emulsion: effects on boron release and decay and termite resistance. Int Biodeter Biodegr 60(3):189–19610.1016/j.ibiod.2007.03.002 ↗
24. Rowell RM (2012) Handbook of wood chemistry and wood composites. CRC Press, London10.1201/b12487 ↗
25. Gindl W, Hansmann C, Gierlinger N, Schwanninger M, Hinterstoisser B, Jeronimidis G (2004) Using a water-soluble melamine-formaldehyde resin to improve the hardness of Norway spruce wood. J Appl Polym Sci 93(4):1900–190710.1002/app.20653 ↗
26. Matthes R, Nehring H, Dellith W (2002) Wasserglas—Holzschutz im Holzbau. Proceedings Integrierter Umweltschutz im Bereich der Holzwirtschaft. Göttingen, München, pp 104–108
27. Xie Y, Fu Q, Wang Q, Xiao Z, Militz H (2013) Effects of chemical modification on the mechanical properties of wood. Eur J Wood Wood Prod 71(4):401–41610.1007/s00107-013-0693-4 ↗
28. Peng Y, Han Y, Gardner DJ (2012) Southern pine impregnated with silicate solution containing cellulose nanofibrils. Holzforschung 66(6):735–73710.1515/hf-2011-0128 ↗