Sandwich compression of sugi (Cryptomeria japonica) and hinoki (Chamaecyparis obtusa) wood: density distribution, surface hardness and their controllability
Source abstract
Abstract
Abstract The sapwood and heartwood of plantation sugi wood (Cryptomeria japonica), and plantation hinoki (Chamaecyparis obtusa) wood were flat-sawn into timbers, then kiln-dried to a MC level below 12%. These timbers were further processed into specific sizes and wetted on the surfaces, preheated at 150 °C and radially compressed into sandwich compressed timbers. Density distribution, compressed layer(s) position and thickness, surface hardness were investigated. It was demonstrated that sugi and hinoki timbers were both applicable for sandwich compression. By controlling the preheating time, sugi heartwood timber, sugi sapwood timber and hinoki timber can be all sandwich compressed, which resulted in surfaces compressed timbers, interior compressed timbers and center compressed timbers. When sugi timbers were sandwich compressed, density only tremendously increased in the earlywood. The increased density of the compressed sugi earlywood was independent of compressed layer(s) position, compressing distance or annual growth width, while for hinoki timbers compression, density increased both in earlywood and latewood. Surface hardness of the uncompressed sugi sapwood was almost twice of that of the uncompressed sugi heartwood. Surface compression sharply increased the surface hardness of sugi heartwood and sugi sapwood. Interior compression and center compression also contributed to increased surface hardness for the compressed timbers, but to smaller extents. Surface hardness change due to the surface compression was consistent with the surface average density change of timbers. Compression layer(s) position exerted statistically significant effects on the surface hardness, while surface hardness of the compressed wood was almost unrelated to the original density of the used wood or average density of the sandwich compressed wood. However, bigger compressing distance led to bigger surface hardness for the surface compressed wood.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Norimoto M (1993) Large compressive deformation in wood. Mokuzai Gakkaishi 39(8):867–874
2. Liu YX, Norimoto M, Morooka T (1993) The large compressive deformation of wood in the transverse direction. I. Relationships between stress-strain diagram and specific gravities of wood. Mokuzai Gakkaishi 39(10):1140–1145
3. Inoue M, Norimoto M, Tanahashi M, Rowell RM (1993) Steam or heat fixation of compressed wood. Wood Fiber Sci 25(3):224–235
4. Inoue M, Kodama J, Yamamoto Y, Norimoto M (1998) Dimensional stabilization of compressed wood using high-frequency heating. Mokuzai Gakkaishi 44(6):410–416
5. Inoue M, Hamaguchi T, Morooka T, Higashihara T, Norimoto M, Tsunoda T (2000) Fixation of compressive deformation of wood by wet heating under atmospheric pressure. Mokuzai Gakkaishi 46(4):298–304
6. Inoue M, Morooka T, Rowell RM, Norimato M, Englund F (2008) Mechanism of partial fixation of compressed wood based on a matrix non-softening methods. Wood Mater Sci Eng 3(3–4):126–13010.1080/17480270903020347 ↗
7. Udaka E, Furuno T (1998) Heat compression of Sugi (Cryptomeria japonica). Mokuzai Gakkaishi 44(3):218–222
8. Udaka E, Furuno T, Inoue M (2000) Relationship between the set recovery of compressive deformation and the moisture in wood specimens using a closed heating system. Mokuzai Gakkaishi 46(2):144–148
9. Udaka E, Furuno T (2003) Change of crystalline structure of compressed wood by treatment with a closed heating system. Mokuzai Gakkaishi 49(1):1–6
10. Matsumoto A, Oda H, Arima T, Fujimoto N (2012) Effect of hot- pressing on surface drying-set in Sugi columns with pith. Mokuzai Gakkaishi 58(1):23–3310.2488/jwrs.58.23 ↗
11. Adachi K, Inoue M (2006) The technique of wood grain compression. Wood Ind 61(11):510–512
12. Li J, Wu YZ, Ma Y (2011) Functional wood. Science Press, Beijing
13. Inoue M, Norimoto M, Otsuka Y, Yamada T (1991) Surface compression of coniferous wood lumber. III Permanent set of the surface compressed layer by a water solution of low molecular weight phenolic resin. Mokuzai Gakkaishi 37(3):234–240
14. Inoue M, Ogata S, Kawai S, Rowell RM (1993) Fixation of compressed wood using Melamine-Formaldehyde resin. Wood Fiber Sci 25(4):404–410
15. Gabrielli CP, Kamke FA (2010) Phenol–formaldehyde impregnation of densified wood for improved dimensional stability. Wood Sci Technol 44(1):95–10410.1007/s00226-009-0253-6 ↗
16. Adachi K, Inoue M, Kawai S (2005) Deformation behavior of wood by roller pressing. Mokuzai Gakkaishi 51(4):234–24210.2488/jwrs.51.234 ↗
17. Huang RF, Wang YW, Zhao YK, Lu JX, Zhang YM (2012) Sandwich compression of wood by hygro-thermal control. Mokuzai Gakkaishi 58(2):84–8910.2488/jwrs.58.84 ↗
18. Gao ZQ, Huang RF, Lu JX, Chen ZJ, Guo F, Zhan TY (2016) Sandwich compression of wood: control of creating density gradient on lumber thickness and properties of compressed wood. Wood Sci Technol 50(4):833–84410.1007/s00226-016-0824-2 ↗
19. Gao ZQ, Huang RF, Chang JM, Li R (2019) Sandwich compression of wood: effects of preheating time and moisture distribution on the formation of compressed layer(s). Euro J of Wood Wood Prod 77(2):219–22710.1007/s00107-018-1377-x ↗
20. Gao ZQ, Huang RF, Chang JM, Li R, Wu YM (2019) Effects of pressurized superheated-steam heat treatment on set recovery and mechanical properties of surface-compressed wood. BioResources 14(1):1718–143010.15376/biores.14.1.1718-1730 ↗
21. Li R, Gao ZQ, Feng SH, Chang JM, Wu YM, Huang RF (2018) Effects of preheating temperatures on the formation of sandwich compression and density distribution in the compressed wood. J Wood Sci 64(6):751–75710.1007/s10086-018-1758-0 ↗
22. Li R, Huang RF, Chang JM (2019) Effect of hot pressing temperature on the density profile of compressed solid wood. BioResources 14(1):1482–149310.15376/biores.14.1.1992-2012 ↗
23. Wu YM, Qin L, Huang RF, Gao ZQ, Li R (2019) Effects of preheating temperature, preheating time and their interaction on the sandwich structure formation and density profile of sandwich compressed wood. J Wood Sci 65(1):1110.1186/s10086-019-1791-7 ↗
24. Hon DNS, Minemura N (1991) Color and discoloration. In: Hon DNS, Shiraish N (eds) Wood and cellulosic chemistry. Marcell Dekker, New York, pp 395–454
25. JIS Z 2101 (1994) Methods of test for woods. Japanese Standards Association
26. Beard JN, Rosen HN, Adesanya BA (1983) Temperature distribution and heat transfer during the drying of lumber. Dry Technol 1(117–140):17
27. Beard JN, Rosen HN, Adesanya BA (1985) Temperature distribution in lumber during impingement drying. Wood Sci Technol 19(277–286):18
28. Tang YF, Pearson RG, Hart CA, Simpson WT (1994) A numerical model for heat transfer and moisture evaporation processes in hot-press drying—an integral approach. Wood Fiber Sci 26(78–90):19
29. Hrčka R, Babiak M, Németh R (2008) High temperature effect on diffusion coefficient. Wood Res Slovak 53:37–46
30. Fotsing JAM, Tchagang CW (2005) Experimental determination of the diffusion coefficients of wood in isothermal conditions. Heat Mass Transfer 41:977–98010.1007/s00231-005-0621-1 ↗
31. Inoue M, Norimoto M, Otsuka Y, Yamada T (1990) Surface compression of coniferous wood lumber I. A new technique to compress the surface layer. Mokuzai Gakkaishi 36:969–975
32. Kitamori A, Jung K, Mori T, Komatsu K (2010) Mechanical properties of compressed wood in accordance with the compression ratio. Mokuzai Gakkaishi 56(2):67–7810.2488/jwrs.56.67 ↗
33. Takahashi T, Nakayama Y (1995) Wood science series 3-Physics. Kaiseisha-Press, Otsu
34. Rautkari L, Honkanen J, Hill ASC, Ridley-Ellis D, Hughes M (2014) Mechanical and physical properties of thermally modified Scots pine wood in high pressure reactor under saturated steam at 120, 150 and 180 °C. Euro J Wood Wood Prod 72:33–4110.1007/s00107-013-0749-5 ↗