The effects of wetting and scratching pretreatment of veneers on shear strength of binderless plywood made from sugi (Japanese cedar, Cryptomeria japonica)
Source abstract
Abstract
To produce practicable binderless laminated veneer lumber (LVL) and plywood, their water resistance needs to be improved. The objective of this study was to manufacture highly water-resistant binderless plywood from sugi (Japanese cedar, Cryptomeria japonica ), basing on a self-bonding mechanism, without any resins or powders. To achieve this, a pretreatment of wetting and scratching veneers was applied. Two types of wetting conditions, soaking for 12 h, and wetting for 1 min, were examined. Sandpaper or a wire brush was used for scratching. Three veneers were laminated in perpendicular directions and hot pressed at 200–220 °C for 20–45 min using two types of pressing schedule: simple 1-step pressing, or 4-step pressing while gradually increasing the pressure. As a result, whichever wetting time was employed, and regardless of the scratching tool used, plywood could be manufactured with both pretreatments. As the wet shear strength showed a comparable value to dry shear strength, the plywood had high water resistance. The highest wet shear strength was 0.6 MPa, for the plywood made by pretreatment wetting of the surface for 1 min and scratching with a wire brush followed by 1-step pressing at 220 °C for 20 min. This was fairly close to the Japanese Agricultural Standard (JAS) requirement. This study indicated that easy pretreatment and mild pressing conditions achieved a binderless plywood with high water resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Wood Treatment and Properties · Natural Fiber Reinforced Composites · Lignin and Wood Chemistry
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Cristescu C (2006) Bonding of laminated veneers with heat and pressure only. In: Proceedings of the 2nd international conference on environmentally-compatible forest products “Ecowood”, Porto, Portugal, 20–22 September 2006: pp 339–348
2. Cristescu C, Sandberg D, Ekevad M, Karlsson O (2015) Influence of pressing parameters on mechanical and physical properties of self-bonded laminated beech boards. Wood Mater Sci Technol 10(2):205–21410.1080/17480272.2014.999703 ↗
3. Okuda N, Sato M (2007) Finely milled kenaf core as a natural plywood binder. Holzforschung 61(4):439–44410.1515/HF.2007.076 ↗
4. Ando M, Sato M (2010) Evaluation of the self-bonding ability of sugi and application of sugi powder as a binder for plywood. J Wood Sci 56(3):194–20010.1007/s10086-009-1096-3 ↗
5. European Norm EN 314 (2004) Plywood—Bond quality. European committee for standardization, Brussels
6. Japanese Agricultural Standard (2003) JAS for plywood. Japanese Agricultural Standards Association, Tokyo
7. Mansouri HR, Leban JM, Pizzi A (2010) High density panels obtained by welding of wood veneers without any adhesives. J Adhesion Sci Technol 24(8-10, SI):1529–153410.1163/016942410X501061 ↗
8. Ruponen J, Rautkari L, Belt T, Hughes M (2014) Factors influencing properties of parallel laminated binderless bonded plywood manufactured from rotary cut birch (Betula pendula L.). Int Wood Prod J 5(1):11–1710.1179/2042645313Y.0000000054 ↗
9. Rabemanolontsoa H, Ayada S, Saka S (2011) Quantitative method applicable for various biomass species to determine their chemical composition. Biomass Bioenergy 35(11):4630–463510.1016/j.biombioe.2011.09.014 ↗
10. Yonezawa Y, Kayama T, Kikuchi F, Usami K, Takano I, Ogino T, Honda O (1973) Chemical analysis, kraft pulping and papermaking characteristics of the important Japanese woods. Bull Gov For Exp Sta 253:55–99
11. Fackler K, Schwanninger M, Gradinger C, Hinterstoisser B, Messner K (2007) Qualitative and quantitative changes of beechwood degraded by wood-rotting basidiomycetes monitored by Fourier transform infrared spectroscopic methods and multivariate data analysis. FEMS Microbiol Lett 271(2):162–16910.1111/j.1574-6968.2007.00712.x ↗
12. Zaman A, Alen R, Kotilainen R (2000) Thermal behavior of scots pine (Pinus sylvestris) and silver birch (Betula pendula) at 200–230 °C. Wood Fiber Sci 32(2):138–143