Effect of Al2O3 content and swaging on microstructure and mechanical properties of Al2O3/W alloys
Source abstract
Abstract
Abstract Al2O3-reinfored tungsten alloys were fabricated by powder metallurgy method and hot swaging technology. The investigation was made on the microstructure, relative density, nano-hardness and fracture toughness (KIC) of the sintered and swaged Al2O3/W alloys. The swaging process and addition of Al2O3 are beneficial to comprehensive properties of the sintered and swaged alloys. After swaging, the Al2O3/W alloys can achieve the full density. According to the nano-indentation test and three-point bend test, the swaged W-0.25 wt% Al2O3 alloy possesses the highest hardness of 7.02 GPa, the greatest modulus of 435.09 GPa and the maximum fracture toughness of 21 MPa·m1/2. The observation of fracture morphology shows that the recrystallization behavior and grain growth occur above 1400 °C in the swaged pure W alloy, which leads to recrystallization brittleness. At the same time, the microstructure of the swaged W-0.25 wt% Al2O3 alloy does not change apparently.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Advanced TEM characterization of oxide nanoparticles in ODS Fe-12Cr-5Al alloys10.1007/s10853-016-0111-5 ↗
2. Radiation stability of nanoclusters in nano-structured oxide dispersion strengthened (ODS) steels10.1016/j.jnucmat.2012.11.021 ↗
3. Fabrication of high temperature oxides dispersion strengthened tungsten composites by spark plasma sintering process10.1016/j.ijrmhm.2009.03.003 ↗
4. Nanostructured yttria dispersion-strengthened tungsten synthesized by sol–gel method10.1016/j.jallcom.2015.10.059 ↗
5. Eliminating bimodal structures of W-Y2O3 composite nanopowders synthesized by wet chemical method via controlling reaction conditions10.1016/j.jallcom.2018.09.310 ↗
6. Effect of ZrO2 content on microstructure and mechanical properties of W alloys fabricated by spark plasma sintering10.1016/j.ijrmhm.2018.11.006 ↗
7. Observations on the ductile-to-brittle transition in ultrafine-grained tungsten of commercial purity10.1016/j.msea.2008.07.074 ↗
8. The effect of yttrium oxide on the sintering behavior and hardness of tungsten10.1007/BF03027538 ↗
9. Preparation, microstructure, and constitutive equation of W-0.25 wt% Al2O3 alloy10.1016/j.msea.2018.12.001 ↗
10. Fracture strength and microstructure of ODS tungsten alloys10.1016/j.ijrmhm.2010.05.009 ↗
11. Synthesis of nanosized composite powders via a wet chemical process for sintering high performance W-Y2O3 alloy10.1016/j.ijrmhm.2017.09.001 ↗
12. Mechanical properties and microstructural change of W-Y2O3 alloy under helium irradiation
13. W-2 wt.%Y2O3 composite: microstructure and mechanical properties10.1016/j.msea.2012.01.011 ↗
14. Effect of high temperature swaging and annealing on the mechanical properties and thermal conductivity of W-Y2O310.1016/j.jnucmat.2015.04.050 ↗
15. Fabrication, mechanical properties and electrical conductivity of Al2O3 reinforced Cu/CNTs composites10.1016/j.jallcom.2018.12.222 ↗
16. Characterization of hot deformation behavior of nanosized Al2O3 reinforced Al6061 composites10.1166/jnn.2019.16144 ↗
17. Tensile properties and strengthening effects of 6061Al/12 wt%B4C composites reinforced with nano-Al2O3 particles10.1016/j.jallcom.2018.07.072 ↗
18. A simple phenomenological approach to nanoindentation creep10.1016/j.msea.2004.04.070 ↗
19. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
20. Fracture toughness investigations of tungsten alloys and SPD tungsten alloys10.1016/j.jnucmat.2007.03.079 ↗
21. Fracture toughness and fracture mechanisms in Mo5SiB2 at ambient to elevated temperatures10.1016/j.intermet.2013.02.008 ↗